    @djwmunro 2 дні тому +2

    Amazing the tube didn’t fail at the factory weld.

    • @samanthamackie1892
      @samanthamackie1892 2 дні тому +3

      the welded areas are actually stronger thats why. its likely the heat affected zone HAZ or the tube being thinner in that spot that caused the failure

    • @samueldoss2464
      @samueldoss2464 День тому +1

      Heat affected zone.