You are the man! I tried refinement using led and ended up vaporizing 9 grams of gold. It took me months to get that much. Well, lesson learned. I hope one day I can be as good as you are!
Every time I see urea get added I see money out the window for the volume you guys process on this channel. You should be dissolving gold bearing material until the reaction stops, saving leftovers for future batch and precipitating used up solutions. Love the content!
I appreciate all of the hard work you do on your Channel I have learned so much from you and still learning, it's been and is one heck of a experience thank you so much job well done I
A pro of living in his country. A con living in Aus, UK. Trinity isnt much for incremental Nitric dosing and conservation of acids... Though it is ewaste and the yields are less certain... and like you said cheap acid. Saves times, seems to be effective. My question is for the cheapskates, me, or those who have difficulty getting their hands on Nitric Acid.
Maybe just snippin the legs as they are still on board would be faster, then just first AR should deal with rest. On cheap nitric: Spectracide Stump-out has a mostly potassium nitrate version. You can cheaply make up to around 40% hno3 without fractile distilling. i think Nilered had a video. Another thing to consider; instead of diluting 70% expensive nitric, use already dilute nitric for all but neccessary. For example i wouldn't recommend using 70% for silver recovery, if your first step is add water the same volume in water.
Are you using distilled water i would hope so as the chlorine will compromise the solution quite a bit.. also id heat the solution because heat helps with the extraction process even further. Basically nice and easy so you get a better yield for your intent and time
I also use tap water. boiling water for 15 minutes will remove all of the chlorine form tap water. Alternatively, leave a bucket of water uncovered at room temperature for at least 24 hours and the chlorine will evaporate without boiling.
I just recently finished a batch of 8000 gold legged transistors. I was surprised at how low the recovery really was. I suppose this helps me know I was not really that far off. Not much in the stock pot I guess.
Actually you need distilled water otherwise need to add sulfuric acid -H2SO4 to eliminate any lead present from the solution. Quite common in most tap waters
You are the man! I tried refinement using led and ended up vaporizing 9 grams of gold. It took me months to get that much. Well, lesson learned.
I hope one day I can be as good as you are!
Every time I see urea get added I see money out the window for the volume you guys process on this channel. You should be dissolving gold bearing material until the reaction stops, saving leftovers for future batch and precipitating used up solutions. Love the content!
Great video , glad I’ve already started collecting these for future refining
Almost 1g per kg material, very nice return. Just a long time to collect 1kg 😎🤙🏼🍺
I appreciate all of the hard work you do on your Channel I have learned so much from you and still learning, it's been and is one heck of a experience thank you so much job well done I
✌️✌️🥰
Nice dude...I'm fron India
Trini cadave son mas peqeñas las pepes. Escasea asta el oro en estos tiempos. El videojenial como todos saludos desde españa😊😜
Your machine grind how many watt sir ???
Nice Vidio
Hello, I am a follower of your channel, could you tell me what are the concentrations of the acids used, HCl and HNO3? Please.
Is there any reason you cannot use CuCl2, aside from it taking longer, to chew out the base metal legs?
Great vid Trinity. Thanks
The guy has loads of cheap acids.
A pro of living in his country.
A con living in Aus, UK.
Trinity isnt much for incremental Nitric dosing and conservation of acids...
Though it is ewaste and the yields are less certain... and like you said cheap acid. Saves times, seems to be effective.
My question is for the cheapskates, me, or those who have difficulty getting their hands on Nitric Acid.
Maybe just snippin the legs as they are still on board would be faster, then just first AR should deal with rest. On cheap nitric:
Spectracide Stump-out has a mostly potassium nitrate version. You can cheaply make up to around 40% hno3 without fractile distilling.
i think Nilered had a video.
Another thing to consider; instead of diluting 70% expensive nitric, use already dilute nitric for all but neccessary. For example i wouldn't recommend using 70% for silver recovery, if your first step is add water the same volume in water.
I snip the legs as a secondary process already. Thanks for the tips though.
@@NOFX0890 Poor man's AR/ nitric . Works every time. All you need is pool acid (HCL) and potassium nitrate(fertilizer).
Why dont you put smb in the solution salt form?
Wow superb
Thanks 🤗
Mantap
Nice..Thanks👍❤👍
If you 1/2 ml of sulfuric to your aqua regia it will remove any lead that was disolved in the process.
Are you using distilled water i would hope so as the chlorine will compromise the solution quite a bit.. also id heat the solution because heat helps with the extraction process even further. Basically nice and easy so you get a better yield for your intent and time
I also use tap water. boiling water for 15 minutes will remove all of the chlorine form tap water. Alternatively, leave a bucket of water uncovered at room temperature for at least 24 hours and the chlorine will evaporate without boiling.
Very good👍👍👍👍
Thank you very much
Is it the one with yellow feet or the one with white feet?
I just recently finished a batch of 8000 gold legged transistors. I was surprised at how low the recovery really was. I suppose this helps me know I was not really that far off. Not much in the stock pot I guess.
You really counted 8000 transistors?
Did you weigh the 8000 transistors? If so, what was your gold yield from that many?
@@scrapping4shiba I did not weigh them, or count them. It was a sealed, labeled bag of new non installed pieces. The yield was 2.2 grams.
Well done 🌟 🌟 🌟 👍
✌️✌️
Super.
Super
1 gram per kilogram. Good yield. Best to just mix them with other ICs.
excellent 👍👍
✌️✌️
My dear sir ask you my mobile phone low great gold pin if you can do the right thing by watching any of your videos please let me know
super..laikos..
2:45 cursed marshmallows
Bóng bán dẫn à Add?
Why you use sulfuric acid?
These have gold too? God golds every where!
Indeed
👍
✌️✌️
Kenapa tidak memakai bahan kimia HF mister?
This24 carret gold
Sir I can use every water or just use stilling water?
Any water
Actually you need distilled water otherwise need to add sulfuric acid -H2SO4 to eliminate any lead present from the solution. Quite common in most tap waters
Ayo bos konten iridium proses
Dear sir is this plated or Gold wire bond?
Inside gold wire bond a Little...
Colour tv aney tv board available this
Yes, also in cell phone charger pcb..
They are in most older and some newer electronics.
how can extract silver .
Dear Sir what meant by 68% of HNO3. PLS Tell me
68% of Nitric acid by mass in aqueous solution means that 68g of Nitric acid present in 100g of solution.
We have hydrochloric acid that has yellow color it has problem?
No problem
Sorry we can use water or just use distilled water?
Just normal water ...
@@TrinityGoldRecovery it is not need distilled water?
Dear sir,any type of transistor contain gold
I think so...
Which we use sulfuric acid ?
For growing up temperature ...
@@TrinityGoldRecovery which percentage we can use sorry we have not high percentage sulfuric acid. We can use sulfuric acid battery
Where is silver, how much?
In deutsch gesprochen wäre es besser
Mantap