Resin with baby powder to fill in layer lines! That right there is an incredibly, mind-blowing tip. All cos-players watching this should thank you profusely, buy you some coffee!
The result is just amazing! I love how 3D printing is like 15-20% of the total time. Really shows that the really important part is indeed craftsmanship.
What i get from watching this video is with determination and practice you can achieve anything and expired resin still work well and i don't need to throw it away,awesome.
Outstanding Walk through video! Thank you so much for producing. You are one of the only 3D Print artists that mentioned ensuring you captured the micro plastics! This in itself is admired. x from New Zealand.
ive used the superglue and baking soda as filler trick before on joints but baby powder and uv resin sounds great, cant wait to try that , i bet its much easier to sand
You are talented. You asked if it was worth it. One of my granddaughters is BIG into StarWars. If I had the equipment and talent, yes it’s worth it. Thank You
Looks absolutely great, like a prop from the Movies. The only thing missing is a little weathering for the used Star Wars look, but that's a matter of taste. 😁
This looks awesome, your hard work really paid off. A few years ago I tried my hand at electroplating 3d prints, I did one Star Trek Holo-emitter in nickel, said "wow cool, that was a lot of work and really messy" and then gave up. If I ever had a big project that required mirror finish metallic surfaces I might try again
I can't believe you used 6 year old expired resin specifically in the hopes it would be yellow due to being expired and having to deal with the "problem" that despite its expiration it turned out "perfectly" against your hopes. Quite amusing.
4:21 TEN?! 5:24 Okay, that's funny. 5:59 I get jealous every time I see this kind of finish. I would love to try to attempt this kind of work one day. 10:28 I know... I knoooooow!
Absolutely fantastic! As always! No idea why anyone would give it a thumbs down. I just checked the pricing of the 5 liter acidic copper plating solution you're using... And you need 10 of them. Pfew! I hope the manufacturer is sponsoring your channel. Thumbs up from me!
Thanks for the great video! Lots of practical information, adding the time it takes for the steps is very useful. The proof that it works is shown and looks amazing. Many thanks.
Gorgeous! Very cool technique. That magical little tiny power sander you used at 6:06 is going to be a game changer for me, though. I've wanted something like that for years, for fine detail sanding of complex parts. Never found one before. Thanks for the link!
Would love to see a video maybe on things that can go wrong during the plating process, and how best to avoid them. Also, I've never had much success with sanding as the layer always starts to peel off before I can get to the higher grit sand papers. Maybe I just need to go gentler as the pieces spend a long time in the bath so I don't think the thickness is the issue.
I always use uv resin and baby powder on my fdm prints, saves a lot of time. I'm so interested in the electroplating. Have been watching your videos all the time but not took the plunge yet
Wow! Having built a full C3PO myself while using a gold chrome spray can (which you can't touch or put anything over the top!) , I'm so impressed with what you've done, the finish! Are you going to do the whole thing now 😁(I'm currently building a full size R2 as well!). Excellent work! I'm watching your IronMan as well now... I love these tutorials you are doing about electroplating. I want to make some custom jewellery just for fun... Happy making!
Would be great to do a dedicated video teaching to make homemade conductive paints, like the graphite+glue and copper+acetone. And maybe homemade electrolyte liquid as in some places, like mine, neither is easy to find. Cheers!
Beautiful results and thank you x 100 for the video showing your technique! I'm less patient, and the parts where you are polishing it turn me off. I recently tried 3D laser sintering printing in stainless steel, followed by powder coating. It gives me the shiny metal surface. -Frank
Beautiful. My man, can you put together a detailed tutorial of the most basic setup so that beginners like myself with say an Anycubic Photon Mono can cheaply electroplate. With shopping lists and step by step instructions. Thanks in advance.
There are some mirror finish metallic spray paints that have been out for a few years that come surprisingly close to that appearance however. So one may want to do a comparison for surface prep and costs. (I suspect the rattle-can stuff not only saves time, but is likely a lot cheaper.)
Surfaces scale quadratically, Volumes scale in a cubic manner. Doubling the sides of a rectangle you get 2^2 = 4 times the area. Doubling the edges of a cube you get 2^3 = 8 times the volume.
I wouldn't use resin for filler, I found good results from Big Boy car body filler. It is very versatile and easy to use like a 2 part epoxy which sets hard in about 15 minutes ready to sand and paint. I've also used a soldering iron and spare PLA off the roll to fix parts that need strength and then smooth them over while the soldering iron cools down. Definitely turned out great. I would agree with Homer: If something takes a long time to do, it's probably not worth it. But that's just me
Using resin as filler literally takes seconds to harden. And since it's resin on resin, there is no separation and very little to sand. It also utilizes the same materials you already have on hand. I've used resin filler on resin parts for years. Car filler is good if you have large parts to fill where it would take forever to brush in resin. But on small blemishes and seams, resin is 1000% easier and faster and much less fumes.
@@cuthwulf I see. Thanks. Although there's no fumes for car body filler either. I was just looking at the results as it was applied and thought it wasn't very smooth. But if it bonds well with the material (I thought it was PLA so didn't know this) then it's probably going to give a better finish when sanded)
Absolutely incredible! For the small parts do you bother going into blender to calculate the surface area or are you using your experience and guestamating?
This is so cool, love your work 🫣 I have a question as I’m working on a small project myself. For small tiny parts that are SLA printed, what can I do to smoothen the surface?
Hi HEN3DRIK. Amazing work, congrats! After watching your video like 5 times :D I have a question. When you take the part out at 8:03 its matte then on 8:05 is super shiny. What happened? have you changed anything, or you polished in between?
Good catch. I missed a dubbing. the matte is after 1 hour. I wanted to show what it should look like after that time. 8:05 is after 4 hours when the brightner kicked in
@@hen3drik After how many hours does it usually turn from matte to shiny? Do you change anything in the current for that or just keep it constant at 1 A/dm^2?
I collect and recycle spilled liquids and reuse the electrolytes over and over by maintaining them. My electrolytes are still the original ones that I’ve bought back in 2018y
Hi ! Thanks for teaching us! Do you have any recommendation for me? I try to apply the copper conductive paint with an airbrush just like you. I dillute it 2(acetone):1(copper paint). I ensure the surface is prepared and smooth (resin print). But when i brush on the mixture, the painted surface is not as smooth as yours, and electroplating it is far away from mirror glaze. Maybe my airbrush pressure is not enough? (3 bar while painting)
Good morning, my friend. I have been following your work for a long time and I have to congratulate you on your excellent work and very explanatory videos. My question is about the paint you made using copper powder and acetone. Do you have any more information about the copper powder, any specifications, is it electrolytic? I believe this is a question that many people have. Thank you very much.
Hi, I use a commercial conductive copper paint that is very thick and i thin it down to make it airbrushable. This paint is not conductive when applied but when it gets into contact with acid. Then it suddenly becomes super conductive. I have yet to make my own, but that's what I'm trying to cover in the next videos or so. I know that getting conductive copper paint is a hassle when not in the EU, so sticking to DIY conductive graphite paint in the meantime is a good alternative AFAIK
looks amazing is the health risk worth it though? probably not so are there any services like JLC PCB this do this kind of electroplating yet? I wonder how expensive it is or would be
I don't think there is that much health risk, as long as you use basic PPE. The most unhealthy processes in here are sanding, that is easily made safer for your lungs using some kind of particle filter mask; the plating acidic electrolyte that contains a small fraction of sulphuric acid that can again be made safer with the proper gloves; and the resin, which I have never dealt with so I'm not that sure about it but many people handle it when using printers so I guess is not that hard to manipulate. To me, the biggest problems seem to be getting all of the stuff, the money and time consumption. But yes, it's true it would be great if there was some kind of service to do all of the great work!
@@adrw216 Yes but no matter how careful you are you will always get sot exposure That dust goes every and those vapor filters for the 3m masks are all but useless There is a minimal amount of carbon in them I used them to paint my garage and still got sick from the fumes. They do almost nothing
Man how do you get that shine right out the bath? All my electroplates come out rough and i need to wet sand before polishing. Truely you are a master at your craft.
I try to deposit very slow with the correct current and an even electrical field. I maintain the bath that it has no dirt in it and polish the conductive paint carefully before plating
Moin Dude. Thank you for you videos and Time. I want to get startet with elktroplaying myself, to expand my 3D Printing Hobby. Could u maybe make an Updated Full Tutorial vid? I have seen your "Rotary Jig" but no Explanation how its works. Also maybe what Products u use and where to procure them. Maybe also a Vid explaing your Fail´s and how to Problem solve them. Sry for the Request Overload :D Keep up the good Work!
This is probably one of the best replicas of C-3PO Ive ever seen! Well done!
Oh, thank you very much 🙂
likewise. awesome work
It's probably got more time into it than the original costume department put into Anthony Daniels entire outfit...
It's beautiful, a piece of art.
Resin with baby powder to fill in layer lines! That right there is an incredibly, mind-blowing tip. All cos-players watching this should thank you profusely, buy you some coffee!
I appreciate the effort of getting dressed to the nines for a split-second visual gag.
The result is just amazing!
I love how 3D printing is like 15-20% of the total time. Really shows that the really important part is indeed craftsmanship.
What i get from watching this video is with determination and practice you can achieve anything and expired resin still work well and i don't need to throw it away,awesome.
That is outstanding, the final finish looks like it could be a render, great job!
This is AMAZING! You're a living legend!
Love to hear more about the graphite acetone super glue mix
Beautiful work as always
Haven't you noticed? That wasn't super glue. It was Gorilla Glue Clear packed into "super glue style" tubes.
Maan, you are crazy! This piece is stunning. Great job!
thanks 😊
Outstanding Walk through video! Thank you so much for producing. You are one of the only 3D Print artists that mentioned ensuring you captured the micro plastics! This in itself is admired. x from New Zealand.
What do you do with the micro plastics when you catch them?
It's amazing the finish you achieved, it really looks like a piece of solid metal and just like in the movie really.
Thank you. I was really surprised how well it looks, feels and sounds (!), as it’s practically metal now
I think it's only a matter of time until you will have built entire C-3PO. Absolutely amazing work.
Thanks for giving us the paint formula for the copper powder and graphite!
Amazing work!!!! I can honestly say, I'll never make one!!! lol I appreciate your attention to safety and detail. WELL DONE!!!!!!
5:20 made me laugh waaaay harder than I should have. lol
I bought a 3D printer a while ago and haven't wanted to print anything until I saw your video! WOW!
Thank you so much for your videos, it's so mind-blowing to see things like this come to reality
Great video. Glad to see your channel has grown so much since I last saw it. Congrats
ive used the superglue and baking soda as filler trick before on joints but baby powder and uv resin sounds great, cant wait to try that , i bet its much easier to sand
You are talented. You asked if it was worth it. One of my granddaughters is BIG into StarWars. If I had the equipment and talent, yes it’s worth it. Thank You
This is nothing short of amazing... WOW!
Looks absolutely great, like a prop from the Movies. The only thing missing is a little weathering for the used Star Wars look, but that's a matter of taste. 😁
Moin, gute Arbeit alter! Sieht wirklich überzeugend aus!
Moin, danke!
This looks awesome, your hard work really paid off. A few years ago I tried my hand at electroplating 3d prints, I did one Star Trek Holo-emitter in nickel, said "wow cool, that was a lot of work and really messy" and then gave up. If I ever had a big project that required mirror finish metallic surfaces I might try again
Had exactly the same results and thoughts when i started. ;-)
Just upped the bar again! This is absolutely GORGEOUS
Thank you, glad you like it!
Looks amazing! Can't imagine all the iterations to get to that mirror finish
Amazing as always!! Well done!
Love your stuff man! Inspiring videos and projects. I always look forward to what you craft next! Keep it up homie
Absolutely perfect! Great job!
I can't believe you used 6 year old expired resin specifically in the hopes it would be yellow due to being expired and having to deal with the "problem" that despite its expiration it turned out "perfectly" against your hopes. Quite amusing.
Moin from Hamburg. The results look fantastic.
4:21 TEN?!
5:24 Okay, that's funny.
5:59 I get jealous every time I see this kind of finish. I would love to try to attempt this kind of work one day.
10:28 I know... I knoooooow!
It looks truly amazing.
I was already obsessed with your work.. now I’m fanatically obsessed! 😍😍😍 so beautiful!
😅 I’m just a dude with electrolyte and sanding paper, seriously!
Well done this looks amazing and thank you for exposing me to plating
Absolutely fantastic! As always! No idea why anyone would give it a thumbs down. I just checked the pricing of the 5 liter acidic copper plating solution you're using... And you need 10 of them. Pfew! I hope the manufacturer is sponsoring your channel. Thumbs up from me!
Wow, incredible!!!
Thanks for the great video! Lots of practical information, adding the time it takes for the steps is very useful. The proof that it works is shown and looks amazing. Many thanks.
Beautiful! Thank you for sharing your work.
Sooo happy you are back!!!!
Wow - looks fantastic!
Looking absolutely amazing.
Impressive! It just doesn´t look 3D printed anymore in the end. So, I´d argue it can totally be worth it.
Man you have crazy level talent your creation out of the world
Thanks!❤️
Wow..really amazing job, thanks for sharing...I need to make this for my humanoid robot parts...😊
Gorgeous! Very cool technique. That magical little tiny power sander you used at 6:06 is going to be a game changer for me, though. I've wanted something like that for years, for fine detail sanding of complex parts. Never found one before. Thanks for the link!
Yeah, there is actually a battery powered Japanese thing : Artima 7. but I couldn’t get it here.
HELL YEAH IT'S WORTH IT!!! IT'S FREAKING AMAZING!!! GREAT WORK!!! 💯🤯
Would love to see a video maybe on things that can go wrong during the plating process, and how best to avoid them. Also, I've never had much success with sanding as the layer always starts to peel off before I can get to the higher grit sand papers. Maybe I just need to go gentler as the pieces spend a long time in the bath so I don't think the thickness is the issue.
Amazing print quality from the x1c pla print
Ooh, someone upgraded their production quality.
I always use uv resin and baby powder on my fdm prints, saves a lot of time. I'm so interested in the electroplating. Have been watching your videos all the time but not took the plunge yet
Wow! Having built a full C3PO myself while using a gold chrome spray can (which you can't touch or put anything over the top!) , I'm so impressed with what you've done, the finish! Are you going to do the whole thing now 😁(I'm currently building a full size R2 as well!). Excellent work! I'm watching your IronMan as well now...
I love these tutorials you are doing about electroplating. I want to make some custom jewellery just for fun...
Happy making!
Thanks! 😃
Brilliant as always!
thankyou for share your knowledge
I learned so much stuff from youtubers, it's time to give back 😅
Great result. You can make a Terminator head as well 👍
Would be great to do a dedicated video teaching to make homemade conductive paints, like the graphite+glue and copper+acetone. And maybe homemade electrolyte liquid as in some places, like mine, neither is easy to find. Cheers!
It's stunning work sire
It's nice to see I'm not the only one who ignores resin expiration dates!🙈
Best one yet!
Thank you
very cool! nice work
That is amazing 👏
thats fantastic
Beautiful results and thank you x 100 for the video showing your technique! I'm less patient, and the parts where you are polishing it turn me off. I recently tried 3D laser sintering printing in stainless steel, followed by powder coating. It gives me the shiny metal surface. -Frank
NOW YOU CAN MAKE DAFT PUNK!
brilliant
OTTIMO VIDEO! COMPLIMENTI
great job
Looks really easy lol!
Great video! You've inspired me to make a 3d printed Tesla coil toroid and give Electroplating a try
🫶
Beautiful. My man, can you put together a detailed tutorial of the most basic setup so that beginners like myself with say an Anycubic Photon Mono can cheaply electroplate. With shopping lists and step by step instructions. Thanks in advance.
Fantastic video, great story telling. I really enjoyed watching it!
02:09, 03:00 and 05:22 are my favourite scenes :D
Thank you, did you recognize the trilobite from Nederland? 😅
@@hen3drik I did! Was the glue the one from Microcenter?
@@JanTec3D eagle eye, it was!
brillliant
Glorious
There are some mirror finish metallic spray paints that have been out for a few years that come surprisingly close to that appearance however. So one may want to do a comparison for surface prep and costs. (I suspect the rattle-can stuff not only saves time, but is likely a lot cheaper.)
Surfaces scale quadratically, Volumes scale in a cubic manner. Doubling the sides of a rectangle you get 2^2 = 4 times the area. Doubling the edges of a cube you get 2^3 = 8 times the volume.
You're absolutely right.
Amazing!
I wouldn't use resin for filler, I found good results from Big Boy car body filler. It is very versatile and easy to use like a 2 part epoxy which sets hard in about 15 minutes ready to sand and paint. I've also used a soldering iron and spare PLA off the roll to fix parts that need strength and then smooth them over while the soldering iron cools down.
Definitely turned out great.
I would agree with Homer: If something takes a long time to do, it's probably not worth it. But that's just me
Using resin as filler literally takes seconds to harden. And since it's resin on resin, there is no separation and very little to sand. It also utilizes the same materials you already have on hand. I've used resin filler on resin parts for years. Car filler is good if you have large parts to fill where it would take forever to brush in resin. But on small blemishes and seams, resin is 1000% easier and faster and much less fumes.
@@cuthwulf I see. Thanks. Although there's no fumes for car body filler either. I was just looking at the results as it was applied and thought it wasn't very smooth. But if it bonds well with the material (I thought it was PLA so didn't know this) then it's probably going to give a better finish when sanded)
Does anyone know where I can get that copper paint in the US?
Always excellent vids. BTW what is the actual current formula for argument of m2?
Absolutely incredible! For the small parts do you bother going into blender to calculate the surface area or are you using your experience and guestamating?
Blender. Always.
This is so cool, love your work 🫣 I have a question as I’m working on a small project myself. For small tiny parts that are SLA printed, what can I do to smoothen the surface?
that's a good question. Maybe using filler primer and throwing the in a tumbler.
sick af
TREMENDO TRABAJO gracias por compartir, espero q sigas haciendo videos te esperamos
Isn’t it easier to use conductive pla for plating? Could you do a how to video in how to electroplate with conductive pla?
It is absolutely worth it, and I would do it but with my 3d printers I have no more room for a chemical lab.
Incredible
Hi HEN3DRIK. Amazing work, congrats!
After watching your video like 5 times :D I have a question.
When you take the part out at 8:03 its matte then on 8:05 is super shiny. What happened? have you changed anything, or you polished in between?
Good catch. I missed a dubbing. the matte is after 1 hour. I wanted to show what it should look like after that time. 8:05 is after 4 hours when the brightner kicked in
@@hen3drik After how many hours does it usually turn from matte to shiny? Do you change anything in the current for that or just keep it constant at 1 A/dm^2?
@@kedo87 Start 0.5* the first 30 min. It usually becomes shiny after 2-3 hrs
Great, thanks for the hint!! Gonna try asap :-)
I love every video you upload!
The Glaive from Krull?
The copper powder mixed with acetone layer is to create a conductive surface so the copper from the plates could stuck on it?
It's amazing. I have some questions, can you help me? Please
How are the liquids disposed of? Can the liquid be reused? for how long?
I collect and recycle spilled liquids and reuse the electrolytes over and over by maintaining them. My electrolytes are still the original ones that I’ve bought back in 2018y
Hi ! Thanks for teaching us!
Do you have any recommendation for me? I try to apply the copper conductive paint with an airbrush just like you. I dillute it 2(acetone):1(copper paint). I ensure the surface is prepared and smooth (resin print). But when i brush on the mixture, the painted surface is not as smooth as yours, and electroplating it is far away from mirror glaze. Maybe my airbrush pressure is not enough? (3 bar while painting)
It takes practice. Try lowering the pressure. Dilute more. Try different angles while spraying.
Amazing!!! 😍 Please put the materials and steps in a list 🙏🏻 I'm no good I English so it's a little difficult to understand 😅
Good morning, my friend. I have been following your work for a long time and I have to congratulate you on your excellent work and very explanatory videos. My question is about the paint you made using copper powder and acetone. Do you have any more information about the copper powder, any specifications, is it electrolytic? I believe this is a question that many people have. Thank you very much.
Hi, I use a commercial conductive copper paint that is very thick and i thin it down to make it airbrushable. This paint is not conductive when applied but when it gets into contact with acid. Then it suddenly becomes super conductive. I have yet to make my own, but that's what I'm trying to cover in the next videos or so. I know that getting conductive copper paint is a hassle when not in the EU, so sticking to DIY conductive graphite paint in the meantime is a good alternative AFAIK
Could you put a general price tag for a setup to achieve such results with electro plating ? (Not accounting for printers)
looks amazing
is the health risk worth it though? probably not
so are there any services like JLC PCB this do this kind of electroplating yet?
I wonder how expensive it is or would be
I don't think there is that much health risk, as long as you use basic PPE. The most unhealthy processes in here are sanding, that is easily made safer for your lungs using some kind of particle filter mask; the plating acidic electrolyte that contains a small fraction of sulphuric acid that can again be made safer with the proper gloves; and the resin, which I have never dealt with so I'm not that sure about it but many people handle it when using printers so I guess is not that hard to manipulate. To me, the biggest problems seem to be getting all of the stuff, the money and time consumption. But yes, it's true it would be great if there was some kind of service to do all of the great work!
@@adrw216 Yes but no matter how careful you are you will always get sot exposure
That dust goes every and those vapor filters for the 3m masks are all but useless
There is a minimal amount of carbon in them
I used them to paint my garage and still got sick from the fumes.
They do almost nothing
Man how do you get that shine right out the bath? All my electroplates come out rough and i need to wet sand before polishing. Truely you are a master at your craft.
I try to deposit very slow with the correct current and an even electrical field. I maintain the bath that it has no dirt in it and polish the conductive paint carefully before plating
Do you have an exact measurement for the graphite paint? I've been trying to get mine right and the paint just flakes or rubs off after drying
Yes: It’s 40g acetone, 2G gorilla glue, 5g graphite.
Moin Dude. Thank you for you videos and Time. I want to get startet with elktroplaying myself, to expand my 3D Printing Hobby. Could u maybe make an Updated Full Tutorial vid? I have seen your "Rotary Jig" but no Explanation how its works. Also maybe what Products u use and where to procure them.
Maybe also a Vid explaing your Fail´s and how to Problem solve them.
Sry for the Request Overload :D
Keep up the good Work!
Seconds after i post that i see that most of that is in the Discription... welp.
Now make a full suit!
Beautiful! Is this how they did the original costume? What is the cost for all parts and processes? Can anyone afford this? :)