And this is why you check every motor with a file to see if it is not Aluminium wire. There was way to much dross for it to all be copper, Now you have made Aluminium-Bronze, no way to tell the ratio unfortunately. Looks very nice though, keep it separate for when you want to cast something in a shiny golden metal. Also: 2:17 that is a VERY fast way to take out the core, I always used to gently tap out the core using a small punch on the sides. From now on I'm doing it this way 😁👍
Nice collection you got there 👍
Pěkná práce
And this is why you check every motor with a file to see if it is not Aluminium wire. There was way to much dross for it to all be copper,
Now you have made Aluminium-Bronze, no way to tell the ratio unfortunately. Looks very nice though, keep it separate for when you want to cast something in a shiny golden metal.
Also: 2:17 that is a VERY fast way to take out the core, I always used to gently tap out the core using a small punch on the sides. From now on I'm doing it this way 😁👍
Welcome to the devil forge community 😂😂
Pozdrawiam serdecznie z Polski 🇵🇱 🤗 good job 👍👍👍
Hey buddy what kind of bit your using?
Hey, which Bit are you referring to
What's the cardboard for? 😂
keeps the crucible from sticking to the bottom
add borax for better skim
How many MPa for copper? 😂
0,12 mpa
Y U NO ALWAYS PREHEAT YOUR MOLD?! 🤬
Hello.
I always preheat my molds and my tools.
I must have forgotten to film it and so it won't be in my video.
@BigstackD
Who doesn't love Mr @BigstackD