How to Solder half round lead coated copper gutters. norwalk Ct by Franklin custom copper works llc

Поділитися
Вставка
  • Опубліковано 17 кві 2013
  • Follow me on instagram @Franklincustomcopperworks Norwalk ct 203 9978069

КОМЕНТАРІ • 131

  • @robvigeant464
    @robvigeant464 5 років тому +4

    Dude, you’re a beast!
    I am a roofing contractor for 25 years and do most everything but never soldering copper because my skills were needed elsewhere.
    I am now learning and researching and have an eye and appreciation for good workmanship... you sir are highly skilled, bravo!

  • @denverscott37
    @denverscott37 2 роки тому +3

    The second pass he's doing is the lacing.. I do box gutters for a living, I solder everyday, first I sweat the seam to draw the solder under the seam, then I lace over top of the seam a second pass, to lace the seam..
    Looked like a pro job to me in this video👍👍

    • @onetwothree4148
      @onetwothree4148 Рік тому +1

      Lacing is unnecessary. I rarely see it in historical work. The problem is people like this guy aren't preheating the copper before they drop the solder. He probably has to lace because his joints fail when he doesn't. The solder doesn't bond well to cold copper.
      Also, if you're not soldering on top of a wood deck, it's faster and better to use a torch instead of an iron. The iron takes several minutes to heat up, then you have to heat the copper up. Ironing is more fool proof though because you can't overheat the copper with it.

    • @denverscott37
      @denverscott37 Рік тому

      @@onetwothree4148 If it's a fold lock I'll only sweat it, but if I've pierced the metal with a drill for a pop rivet then I'll actually lace it. I think the lacing is more just kinda putting your signature on your work.

    • @onetwothree4148
      @onetwothree4148 Рік тому +1

      @@denverscott37 I mean, thicker solder is stronger. But lacing is mostly cosmetic. I'd rather heat the copper properly on my first pass. I do go back over and add more solder after, if it's a thick joint, but I usually do it evenly, rather than leaving stitches. Some of these videos on here show people stitching dirty copper. That won't be a strong bond at all

  • @smsmetal
    @smsmetal 10 років тому +12

    @ Patrick Martin AGREED !!!!!!!! Soldering 101 ……First day "sweat/sweating" "capilary action" more material to material to soldering copper contact insuring heat transfer to achieve capilary action resulting in a superoior soldered joint.
    I must say with some hesitation ….? The work & soldering LQQKs better than 75% of whats out there "accepted" as high end work/craftsmanship in todays work force. :-/

    • @phrodendekia
      @phrodendekia 5 років тому

      Yep. Insctincts say soldering is the way it must be done.

    • @jfmc2581
      @jfmc2581 5 років тому +1

      Yep Terrible job! this guy is just gunking the solder globs on the outside!! This is a horrible job!!
      Looks pretty though kinda like a weld but it didn't get between the metal to form a bond. Amazed that they published this as if it was a good job!!

    • @jims5656
      @jims5656 5 років тому

      google a stitch or lace for solder...rookie comment there dude. the biggest problem in video is lack of pre-tin prep and sweat solder before applying the lacing.

  • @jodybailey88130
    @jodybailey88130 8 років тому +4

    Very nice job Frank. Where do I get a torch solder iron? Also, What kind of cleaner and solder do you use?

  • @leandrogomez6609
    @leandrogomez6609 2 роки тому +1

    Una obra de arte , saludos !!!!

  • @lionelhernandez34
    @lionelhernandez34 2 роки тому +2

    Been in this industry for a very long time, part of the reason I stick with it is there's so many different ways of doing things. I consider it every learning myself, why a second lap? Not bashing just curious, here in central Texas it's more of a sweat technique. If I had to label yours I'd call it a stitch atop a sweat. For strength I would assume, appreciate you sharing your skill.

    • @denverscott37
      @denverscott37 2 роки тому +1

      Sweat and lace , that's how I do my seams in box gutters. The sweat draws the solder under the seam and the lace covers the seams afterwards, just for strength. I also use steel pop rivets on all my seams. .

    • @lionelhernandez34
      @lionelhernandez34 2 роки тому +2

      @@denverscott37 definitely nice work, we've always riveted our joints in all honesty galvanized has pretty much been replaced with painted steel and galvalume so we've been using raw or painted stainless to minimize rust. Copper of course is usually stainless or brass mandrel with copper head, so few contractors utilize quality fasteners these days.

    • @denverscott37
      @denverscott37 2 роки тому +1

      @@lionelhernandez34 I usually use ReziBond galvanized for pretty much all my metal work. It's slightly easier to use than the heavier guage stuff and I get nice clean bends on the sheet metal break with it. I miss the old terne metal we used to use back when I started 30 years ago. Follansbee was the name of the company that made it. They were in business like 150 years, but they closed up shop and stopped producing it for some reason.

  • @fredflintstone2077
    @fredflintstone2077 9 місяців тому

    At last, someone who knows the difference between soldering and welding lead.

  • @danielsexton902
    @danielsexton902 8 років тому +1

    Very cool. I don't see many copper gutters in my area. How long of a piece of gutter can you hang at one time? Do you end up soldering on a ladder when you have really long runs? Or is this limited to short lengths and few corners?(I hang 5" aluminum seamless guttering with corners that are sealed with caulking)

  • @robertruizcampwolfden8579
    @robertruizcampwolfden8579 4 роки тому +5

    There ya go now that’s a pro! Just hold that tip there a few seconds longer on each drip to draw them in like tear drops you got it !

  • @proffesionalthings2662
    @proffesionalthings2662 8 років тому +2

    Nice work

  • @richardmckuhen6661
    @richardmckuhen6661 7 років тому +32

    I appreciate your work, but the iron is pulling the solder where the iron goes. The best soldered joints have the solder sweated into the joint, by heating the area beneath the joint. The solder should be flowing under the outlet lip, with minimal solder piled up on the outside edge. Piling solder on top of solder does not improve a soldered sealed joint of metals. It does make the water pond around the outlet though.

    • @philbox4566
      @philbox4566 6 років тому +2

      Put the downpipe drop underneath the gutter bottom too. No need for any solder then. Just dob the rivets and yer golden.

    • @onetwothree4148
      @onetwothree4148 Рік тому

      100% correct. They are not heating the copper up enough for it to wick under. His solder should disappear into the seam. Throwing hot solder on cold copper is a cold joint. It is a much weaker bond.

  • @bradywilliams2666
    @bradywilliams2666 5 років тому +4

    Clean your iron more often. 1/3 ruby red and 2/3 water solution works great. Also I don't understand the multiple passes. One nice pass that is sweated into the joint is plenty.

    • @frankch25
      @frankch25  5 років тому

      Ok Thanks

    • @frankch25
      @frankch25  5 років тому

      Gracias

    • @mateisztoika3884
      @mateisztoika3884 4 роки тому +1

      it is best to use only a very thin row around the pipe and it would be good to bend your soldering hammer so that you can use it as a shovel. and it would be much better to use a collection tube for the outside of the gutter

    • @kyegebb3735
      @kyegebb3735 3 роки тому

      What is the end bit called?

  • @franciscorochajunior
    @franciscorochajunior 9 років тому +3

    lindo trabajo Franklin

    • @frankch25
      @frankch25  9 років тому

      Gracias por ver mis videos. Me das un like ,,,,

  • @sweeyong7756
    @sweeyong7756 11 днів тому

    Can i use this technique to join the gap seams for stainless gutters? Cheers

  • @NETWizzJbirk
    @NETWizzJbirk 3 роки тому +5

    It looks good, but no need for the second pass. I would have fluxed under the lip then heated the copper pipe with a torch and let it pull in under the lip with capillary action (solder follows heat). I would have inspected underneath to verify the solder pulled all the way around. It would have used less solder, too. Personally, I would probably just use a lead-free plumbing solder, but your 50/50 rod is fine too for gutters. If you really wanted something closer to a weldd, I would braze it with SilPhos DynaFlow (Harris) or SilPhos/StaySilv 15%. That said soft solder is plenty good enough. The best soft solder would probably be StayBrite 8, but it’s overkill. For this even a cheap 95/5 plumbing solder would be superb.

    • @onetwothree4148
      @onetwothree4148 Рік тому

      Soft solder is better for this because it is slightly flexible. He should have cleaned it and torched it though. Irons are for when you're working above wood that could catch fire.

    • @onetwothree4148
      @onetwothree4148 Рік тому

      Also, this video shows you how to make cold joints. He is only heating the solder and he never heats the copper properly. That's probably why he adds an extra pass. The solder does not bond as well if you don't hold the iron on it to heat it up. You can see how the solder bubbles up with ridges where it meets the copper. That's not good.

  • @nikond90
    @nikond90 Рік тому

    Impressive!

  • @reychingon74
    @reychingon74 3 роки тому

    Mu gusta como solda compa..yo tambn soldo pero no tan bien como usted..cuestión de practica creo

  • @larrycrookshanks9091
    @larrycrookshanks9091 3 роки тому

    Great looking job. The caulk junkies should take the time to learn. Then they wouldn't have to redo it.

  • @adamformanack318
    @adamformanack318 2 роки тому +1

    i was trained like this,......hold your breath,...exhaul,.. an make snake skin,...ahahhehe

    • @frankch25
      @frankch25  2 роки тому +1

      👏👏👏👏👏👏

  • @telosfd
    @telosfd 9 років тому +1

    Really nice traditional job i like it.

  • @kyegebb3735
    @kyegebb3735 3 роки тому

    What is the end on the torch please? Looking to buy one

  • @jhanbaldiandbendy8032
    @jhanbaldiandbendy8032 6 років тому +1

    Beautiful work.

    • @jfmc2581
      @jfmc2581 5 років тому

      beautiful and completely wrong!!
      Only looks good to People that don't know what they're doing. He is supposed to be bonding the 2 metals not globbing shiny pretty stuff on the outside this will fail and the short time.

  • @noy_tv2053
    @noy_tv2053 7 років тому +1

    can I ask? what gas you use?

  • @o.pzindal2104
    @o.pzindal2104 5 років тому +1

    Nice

  • @TomCorliss
    @TomCorliss 8 років тому +3

    Beautiful work, why 2 passes around the downspout ? Your work looks so good I would think the first pass woul do. Thanks for the video

    • @billray1785
      @billray1785 7 років тому +2

      I would say the 2nd pass was for strength, might be wrong though.

  • @frankch25
    @frankch25  9 років тому +4

    Happy new year 4 everybody. 2015

  • @rustygoldfanatic8830
    @rustygoldfanatic8830 Рік тому

    Got to be a Chicano. Takes tons of skills if you dont believe me try it.

  • @timbuktu5885
    @timbuktu5885 3 роки тому

    Nice!!!!!

  • @donnies1902
    @donnies1902 6 років тому +10

    Your only sweating a 1/4" lip in copper outlets no need for the two passes. 1 pass with the proper heat in the proper place would of done just fine. Every time you move the iron outside the flange of the outlet your just un-sweating the flange weakening it. More solder doesn't mean a stronger joint.

    • @Astromyxin
      @Astromyxin 4 роки тому +2

      This is what you get when you don't have knowledgeable people who train employees in the correct way to do things, you get baloney like this.

  • @dekonfrost7
    @dekonfrost7 10 років тому +2

    yes it is gold soldering i had hoped when you deposited more solder you would go around and let it infiltrate the joint and carry heat..these are the joints that look pretty but are weak and crack in low temperatures..sorry man..you need to ditch that acetylene man

  • @pigfigjig
    @pigfigjig 2 роки тому

    Sweet

  • @derwikinger_de2903
    @derwikinger_de2903 4 роки тому +1

    Zumindest stehts bemüht :D

  • @chrischoat9099
    @chrischoat9099 7 років тому +1

    Hi rally nice job, what spec solder you use and what flux do you recommend?

    • @frankch25
      @frankch25  3 роки тому

      Brand: La-Co
      4.1 out of 5 stars 24Reviews
      LA-CO M-A Liquid Stainless Steel Flux Liquid

  • @jamesvertin8676
    @jamesvertin8676 7 років тому +2

    copper braiding is good on the Statue of Liberty & on a rooftop chimney caps, but outlets and corners for raingutters are alittle overkill. but still very nice work!

  • @reychingon74
    @reychingon74 3 роки тому +1

    Buen video..yo tambn solo chimeneas pero no soy tan bueno como usted, me seria de mucha alluda unos tips

    • @frankch25
      @frankch25  3 роки тому +1

      Buen dia y felices fiestas. Pues aquí estoy para cualquier ayuda amigo

  • @naoufelmelayh240
    @naoufelmelayh240 4 роки тому +1

    THANKS FOR VIDEO what it the material in galvanized metal , ?

  • @frankch25
    @frankch25  10 років тому +1

    Thanks 4 all comments. Gracias por sus comentarios. Lo tendré presente

    • @JCguttersandconstruction
      @JCguttersandconstruction 7 років тому

      frankch25 Que clase de material es es que está soldando? Esto es lead coated copper?

    • @frankch25
      @frankch25  7 років тому

      Si es ese material

  • @user-cj7yx5ig4b
    @user-cj7yx5ig4b 5 років тому +4

    Им что олова больше некуда девать?)

  • @jaym.4611
    @jaym.4611 5 років тому

    Are you using flux or is this more of a silver solder/brazing application?

    • @frankch25
      @frankch25  5 років тому

      Flux.

    • @frankch25
      @frankch25  3 роки тому

      Brand: La-Co
      4.1 out of 5 stars 24Reviews
      LA-CO M-A Liquid Stainless Steel Flux Liquid

  • @garagekeys
    @garagekeys 7 років тому +1

    Good work, looks great. Is there an epoxy alternative?

    • @onetwothree4148
      @onetwothree4148 Рік тому

      For non-built-in gutters, you could perfectly clean the copper and use pure silicone. It will last decades in direct sun. Not as good as solder, but a surprisingly good option for gutters.

  • @81soriano
    @81soriano 8 років тому +1

    Nice work! I hope you get paid by the hour and not by foot!

  • @granafabrik
    @granafabrik 8 років тому

    Por que pensaba que era un video Alemán y que no sabias español lo siento

  • @stefanegert1752
    @stefanegert1752 5 років тому +1

    Genauso sieht Pfusch aus.Wunderbare kalte Lötstellen.

  • @originalfallinggirl
    @originalfallinggirl 2 роки тому

    Where can I buy that doodad you use to solder and what gas/solder do i use?

    • @frankch25
      @frankch25  2 роки тому +1

      Metro roofing supplier. Stamford Connecticut

  • @roseshkarate4571
    @roseshkarate4571 2 роки тому

    I WANT PURCHASE

  • @frankables3308
    @frankables3308 6 років тому

    Looks like galvanized material with a copper Outlet in hangers not good touching each other

    • @frankch25
      @frankch25  6 років тому +1

      Frank Ables lead coated gutter w/red copper outlet

  • @nebojsastojiljkovic6879
    @nebojsastojiljkovic6879 5 років тому

    E tako se to radi!!! A ne sadasnji majstori spajaju sa silikonom!!!

  • @eduinrodesno7841
    @eduinrodesno7841 2 роки тому

    Que marca es el tip de copper

    • @frankch25
      @frankch25  2 роки тому

      Lead coated copper es él cobre con baño de plomo

  • @granafabrik
    @granafabrik 8 років тому

    Hallo, ich bin Spanisch in ein paar Wochen habe ich Deutschland verlassen Setter Zink und guttering zu arbeiten, gibt es keine Arbeit dieser Arbeit ??

    • @frankch25
      @frankch25  8 років тому

      Si eres de España porque no escribes español???

  • @ManuelHernandez-vr9ft
    @ManuelHernandez-vr9ft 5 років тому

    Dónde compro el cautín???

    • @frankch25
      @frankch25  5 років тому

      Lo venden en metro roofing o la encuentra en eBay

  • @honorepol5425
    @honorepol5425 3 роки тому +1

    Salut, comment s'appelle cette pane?

    • @nonodepanamo4933
      @nonodepanamo4933 2 роки тому

      Je sais qu en Suisse ils sont tous comme ça les fers à souder très pratique pour les angles notamment

  • @lucianoalvarado4839
    @lucianoalvarado4839 6 років тому +1

    Chingon mataran

    • @frankch25
      @frankch25  6 років тому

      Luciano Alvarado gracias pana

  • @fernandojaviergarciamendoz9824
    @fernandojaviergarciamendoz9824 5 років тому

    Como se llama esta herramienta?

    • @frankch25
      @frankch25  5 років тому

      Hola. No entiendo su pregunta?? Si pregunta por la piedra con la que se suelda. La puesdes conseguir en todo lugar que vendan material para techos y cobre

  • @poupsdu7884
    @poupsdu7884 5 років тому

    C’est quoi comme panne ? Une faite maison ?

  • @astaroth120
    @astaroth120 5 років тому

    Силиконом замажьте и все дела . Припой этот также самое через годик сгниет и все потекет

  • @davidsainteve4927
    @davidsainteve4927 6 років тому +2

    Ça ne pose pas de problème à personne ???? Zinc et cuivre..pas bon ménage entre eux....electrolyse.non.
    Sinon beau travail..belle soudure..

    • @grugdominus1540
      @grugdominus1540 5 років тому

      Le cuivre est étamé , ça se voit mdr

    • @Ekyneko
      @Ekyneko 4 роки тому

      Par contre je comprends pas sa façon de souder mdr

    • @Ekyneko
      @Ekyneko 4 роки тому

      Je suppose que c'est pas les mêmes normes qu'ici

    • @yanism9409
      @yanism9409 4 роки тому

      C'est du pas du zinc mais du cuivre etamer

  • @fortunatos4323
    @fortunatos4323 4 роки тому

    Over kill

  • @nishantsoni5378
    @nishantsoni5378 6 років тому

    Which flux

    • @frankch25
      @frankch25  6 років тому

      Nishant Soni LA-CO . M-A FLUX

  • @allrad2190
    @allrad2190 8 років тому +3

    Kupfer auf Zink löten wer hat dir das beigebracht ?

    • @frankch25
      @frankch25  8 років тому

      hallo Freund . Zink ist nicht das Material arbeite ich .... ist Kupfer Schweißen dieser Art führen haben Kupfer zu reinigen eine bessere Schweiß zu haben

    • @frankch25
      @frankch25  8 років тому

      sorry, wenn in Deutsch falsch geschrieben ...

    • @michaelzube7977
      @michaelzube7977 5 років тому

      Pfuschen hoch 10...sowas geht nur im Ausland😲😲😲

    • @Gaynaplgujh
      @Gaynaplgujh 5 років тому

      ist alles aus kupfer nennt sich verzinntes kupfer, in .de kann sich das keiner leisten

  • @larrymaloney877
    @larrymaloney877 3 роки тому +1

    Not getting the parent metal hot enough. You are dobbing solder over the seam-not the best.

    • @MrSolarstu
      @MrSolarstu 3 роки тому +1

      I do love the pro's opinions!!

    • @larrymaloney877
      @larrymaloney877 3 роки тому +1

      @@MrSolarstu , I looked around UA-cam and found this example of most excellent gutter soldering. The work was beautiful-hot enough to flow into one continuous stream of molten solder. Until I saw this pro's work I feared copper gutters were too difficult for the process. This spring I'm installing soldered copper gutters and will use this expert video as a guide.

    • @MrSolarstu
      @MrSolarstu 3 роки тому

      @@larrymaloney877 Are you telling me that now you like it, make your mind up!

    • @larrymaloney877
      @larrymaloney877 3 роки тому +1

      @@MrSolarstu , sorry, I was commenting on another video-did some editing and changed my meaning accidentally. I've seen worse than this demo, but there is much better which is what I meant to reference. This guy isn't getting the parent metal hot enough for smooth-flowing solder. The metal itself should melt & flow the solder, not the iron. If it won't flow touched against the parent metal-the metal isn't hot enough, Keep in mind, the goal is for the molten solder to flow seamlessly between the two copper surfaces. Sorry for confusing the two. Check out a few more and you'll see the difference. I'm a certified welder, and have soldered for years, but never gutters.

  • @user-fd4pv3pj6q
    @user-fd4pv3pj6q 5 років тому

    К етому водостоку еще свенцовую крышу. Я в шоке, какой смысл етих затрат.

    • @frankch25
      @frankch25  5 років тому

      English please

    • @user-oo5ri7sy2k
      @user-oo5ri7sy2k 5 років тому

      @@frankch25 Херея это все и твой энглишь херня полная😂

  • @Dachdeckergeselle
    @Dachdeckergeselle 5 років тому

    Was solln das werden?

  • @johnpreston9574
    @johnpreston9574 3 роки тому +1

    Richard MCK. You sound like a plumber! What he is doing is leaching and stitching! This has been a tried and proven method for over 100 years!

  • @nvennven1053
    @nvennven1053 5 років тому

    Mdr il coûte pas trop cher en étain lui 😂

    • @frankch25
      @frankch25  5 років тому

      English please

    • @poupsdu7884
      @poupsdu7884 5 років тому

      C clair la targette prend une claque

  • @lepadatuchristian6960
    @lepadatuchristian6960 4 роки тому

    Sorry man but this is wrong in so many ways... I don't know even where to start😰

    • @frankch25
      @frankch25  4 роки тому +1

      Ok let me see your jobs. Show me how to solder 🤧🤧🤧🤧

  • @joeldeletre757
    @joeldeletre757 10 років тому +2

    technique de soudure original

  • @mateisztoika3884
    @mateisztoika3884 4 роки тому +1

    You are use to much of material for that "welding" only 1-2 centimeters of that bar are enough for that!
    I'm a gutters and metal roof Master and in that half gutter will stay water because of to much welding an the pipe

  • @methodeman120
    @methodeman120 3 роки тому

    wtf is this??