Thanks. I recently started playing with my paints I ordered. Silly question, do they have to be 100% dry before firing? I am finding they are taking a very long time to air dry. I live on the coast and it’s humid here.
No silly questions. I suggest drying them before firing. I use a heat gun to speed up the drying process. This also helps get rid of some of your mixing medium - I use A-14 for painting, but other mediums for different processes. If you want more info, check out my $5 pdf (it’s worth it!) -jody
3:36 where did u get the beveled glass mixing palette?
We fired 6mm clear glass in the kiln to round the edges.
Thanks. I recently started playing with my paints I ordered. Silly question, do they have to be 100% dry before firing? I am finding they are taking a very long time to air dry. I live on the coast and it’s humid here.
No silly questions. I suggest drying them before firing. I use a heat gun to speed up the drying process. This also helps get rid of some of your mixing medium - I use A-14 for painting, but other mediums for different processes. If you want more info, check out my $5 pdf (it’s worth it!) -jody
@@jodywalker7334 thanks so much. I’ll check it out.
Is this color can be put in kilns
Absolutely. These enamels are specifically made for use in kilns.
Hi, does it works in float and microwave kiln?
Works fine on float, can't say on microwave kiln, depends on how hot and how long the firing.
What do you mix with?
As shown in the video, we use A-14.
Is this color can be put in kilns