why not get the PGM's out first.. cause smb also drops PGM's like palladium.. which is likely why the solution is green.. you're dropping PGM's with gold or use ferrous sulfate and holy hell still nice yeild tho.. only from the bottom parts.. most of the gold is in the tops.. unless you combined them later .. very nice
После отделения подложек от шляпок вес уменьшился раза в два. До 1.5 кГ. Так что нормально он взял. К тому же мосты в корпусе BGA960 и BGA240 отличаются по содержанию в 4 раза. С микса мостов где перемешаны мосты от материнских плат, сетевых роутеров и принтеров получается грамм 5-6 на килограмм исходного материала в виде шапок без подложек.
Can I use 85% pophoric acid + 12.% hydrogen peroxide to dissolve unnecessary metals and then, after filtration of potassium nitrate and hydrochloric acid, to dissolve the gold? The process will be longer, but legal. The question is whether it is effective enough.
The peroxide will dissolve your gold too, atleast with hcl. Not sure whats the use of phosphoric acid. If you can get your peroxide to 30% you can easily dissolve the gold.
phosphoric acid in the presence of hydrogen peroxide (in Europe you can legally buy a maximum of 12%) well dissolves metals such as zinc, aluminum, copper, i.e. basically all brasses and bronzes, as well as pure copper (and it is legal and does not affect gold and other precious metals), then after filtering solution and washing the residues, I am thinking about using potassium nitrate with hydrochloric acid. All these chemical compounds can be legally purchased despite local (in my opinion stupid) Concentrated acids such as nitric acid, sulfuric acid, concentrated hydrogen peroxide and many others are unavailable to private individuals. 
@@robertmischke248 I would use HCL to make a copper chloride solution and get rid of all the base metals then use HCL and peroxide to dissolve the gold. Tip: Use a good freezer and you can purify both hcl and peroxide, only water will freeze, note both of these reactants will be very dangerous after and you dont know what concentration you will get.
Greetings to you my friend Aman, your work is good, perfect and professional. The percentage you got is good, approximately 4.9 grams per kilo. Knowing that there is still a small percentage of gold and silver in the other part of the Ic bga. You lost a good percentage of silver, approximately 30 grams or more.
why not get the PGM's out first.. cause smb also drops PGM's like palladium.. which is likely why the solution is green.. you're dropping PGM's with gold or use ferrous sulfate
and holy hell still nice yeild tho.. only from the bottom parts.. most of the gold is in the tops.. unless you combined them later .. very nice
Awesome.
Iman jan khste nabashi
Jesaratan har kilo BGA ba heat sink v bedun heatsink kiloyi chand b dollar kharidi?
ina tavasote khodemoon az dastgahaye elektroniki jam avari shode doste aziiz
Informative video pal!❤
thanks for watching bro 🌹🌹🌹🌹
Где-то половино спрятал от глаз червивых 😂😂😂много нехватка золота.
thanks for watching
Mega wynik! Nic dziwnego, że BGA są tak chetnie zbierane.
Napisz mi czy tłumaczy UA-cam Tobie moje komentarze?
yes
thanks for watching my videos
Дружище. Ищи потери. Очень мало взял.
После отделения подложек от шляпок вес уменьшился раза в два. До 1.5 кГ. Так что нормально он взял. К тому же мосты в корпусе BGA960 и BGA240 отличаются по содержанию в 4 раза. С микса мостов где перемешаны мосты от материнских плат, сетевых роутеров и принтеров получается грамм 5-6 на килограмм исходного материала в виде шапок без подложек.
thanks 🌹🌹🌹🌹❤️
Beautiful video sir
Thanks a lot
I can't use nitric acid in my country, how can I do this without using nitric acid?
Super video!!!
you can sodyum nitrat + Citric acid
Can I use 85% pophoric acid + 12.% hydrogen peroxide to dissolve unnecessary metals and then, after filtration of potassium nitrate and hydrochloric acid, to dissolve the gold? The process will be longer, but legal. The question is whether it is effective enough.
The peroxide will dissolve your gold too, atleast with hcl. Not sure whats the use of phosphoric acid. If you can get your peroxide to 30% you can easily dissolve the gold.
phosphoric acid in the presence of hydrogen peroxide (in Europe you can legally buy a maximum of 12%) well dissolves metals such as zinc, aluminum, copper, i.e. basically all brasses and bronzes, as well as pure copper (and it is legal and does not affect gold and other precious metals), then after filtering solution and washing the residues, I am thinking about using potassium nitrate with hydrochloric acid. All these chemical compounds can be legally purchased despite local (in my opinion stupid) Concentrated acids such as nitric acid, sulfuric acid, concentrated hydrogen peroxide and many others are unavailable to private individuals.

@@robertmischke248 I would use HCL to make a copper chloride solution and get rid of all the base metals then use HCL and peroxide to dissolve the gold. Tip: Use a good freezer and you can purify both hcl and peroxide, only water will freeze, note both of these reactants will be very dangerous after and you dont know what concentration you will get.
you lost the silver in the ashes. treat the ash with ammonia.
عالی مثل همیشه ❤
ممنون از حمايت شما 🌹🌹🌹🌹
Very useful thanks bro
thanks bro 🌹🌹🌹🌹
Очень мало вышло, бедные мосты
Не согласен. У таких мостов примерный выход 9.5 гр с килограмма. Много таких делал, почти одинаковый результат. Где то потери.
Will be good if you weight top parts before burning. Thanks
Thanks for the suggestion, I'll keep that in mind for future videos. 🌹🌹🌹
Без подложки было 1,5кг? Если да то нормально взял.
yes it is and thanks for watching sir
Greetings to you my friend Aman, your work is good, perfect and professional. The percentage you got is good, approximately 4.9 grams per kilo. Knowing that there is still a small percentage of gold and silver in the other part of the Ic bga. You lost a good percentage of silver, approximately 30 grams or more.
Thanks for watching and for the comments, I'm always trying to improve.
Buz yada soğuk su ile keşke gümüşünü alsaydın
izlediniz için teşekurler efendi
زندگیت همیشه طلایی
ممنونم اقا مهدي گل🌹🌹🌹🌹❤️
Super nice nugget.
thanks for watching bro 🌹🌹🌹🌹
Why don't you bake one more time the ash from the chips hasn't released your 100% gold your raztvotrat was green
thanks for watching sir
Чистый королек
thanks for watching
Bhai ap kis country say hain?
plz rply thanks?
Qual precipitante você usou
sodyum metabisulfit and hydrazin hydrate
Aprox. 0,49 %.
🌺🌺🌺🌹
How to buy hydrazine hydrate
Id rather cement it using copper, or sodium metabisulfate.
Excellent video bro 🎉🎉🎉🎉
Thanks 😁
👍👍👍
thanks for watching sir
🎉🎉🎉🎉
🌹🌹🌹🌹
Waste of time
🙄🙄🙄🙄🙄🙄🙄
This is not a very streamlined process. It also uses chemicals that aren't needed as well as takes much longer than the scientific process.
Hello sir , Can you explain the proper scientific process to recover in a more efficient and scientific way please ? Nice day .
@zibobpompon5768 search for a guy on here called sreetips. His process is congruent to the scientific process. God bless,😉