The Magic Of Citric Acid: How To Passivate In-house

Поділитися
Вставка
  • Опубліковано 20 лип 2024
  • Learn how to passivate your own CNC Machined Stainless Steel Parts.
    Join this channel to get access to perks:
    / @titansofcnc
    Join our community Discord! / discord
    Checkout Stellar Sollutions here: citrisurf.com/
    0:00 DIY Passivation Setup
    1:47 Passivating Stainless Steel
    4:16 Titans of CNC Store
    4:46 Passivation Acid Bath
    7:42 CNC Shop Caught Fire
    8:42 Thank you!
    9:07 Passivated Stainless Steel Parts
    10:44 Bloopers
    Help us fund FREE Education by purchasing tools seen in our videos here:
    TITANSofCNCTooling.com
    Create your free CNCEXPERT profile here:
    rebrand.ly/TiCNCEx
    FREE CNC Machining Academy:
    rebrand.ly/TiAcademy
    FREE Aerospace Academy:
    rebrand.ly/TiAero
    FREE Grinding Academy:
    rebrand.ly/TiGRIND
    Subscribe for daily content and expert knowledge: rebrand.ly/SUBTITANS
    ___
    ___
    Follow us on Instagram:
    rebrand.ly/TiINSTA
    Like us on Facebook:
    rebrand.ly/TiFACEBOOK
    Join the conversation on our Facebook Group:
    rebrand.ly/TiFBGroup
    Connect with us on LinkedIn:
    rebrand.ly/TiLINKEDIN
    ___
    ___
    THANK YOU to our Partners who make this content possible:
    Kennametal - rebrand.ly/TiKennametal
    Heller: us.heller.biz/titansofcnc/
    DN Solutions - www.titansfordn.com/machines
    United Grinding - hubs.ly/Q013zHpC0
    Mastercam - rebrand.ly/MastercamEDUTiYT
    Tornos - bit.ly/3MDcqLh
    Blaser Swisslube - rebrand.ly/TiBlaser
    Solidworks - rebrand.ly/TiSLDWRKS20
    Trumpf - rebrand.ly/TiTRUMPF2022
    Markforged - bit.ly/Titans_Markforged
    Tyrolit - rebrand.ly/TiTYROLIT
    Mitutoyo - rebrand.ly/TiMitutoyo
    Haimer - rebrand.ly/TiHAIMER
    Schunk - rebrand.ly/TiSchunk
    Kaeser Compressors - us.kaeser.com/titan
    #Machining #Machinist #Engineering
  • Наука та технологія

КОМЕНТАРІ • 88

  • @tdg911
    @tdg911 Рік тому +49

    Tyson I’ve said it before and will say it again your videos are always very clear and to the point. You’re a natural. Thank you for bringing us these videos. Much love and gratitude

  • @noahc6544
    @noahc6544 Рік тому +18

    One thing you could look into for the new tank is a literal thermal fuse, since you'll have a lot of water in there it shouldn't need a super high temperature rating

  • @AidenJSS
    @AidenJSS Рік тому +5

    Tyson is the best. Thank you for teaching me something new.

  • @jamiemacdonald436
    @jamiemacdonald436 3 місяці тому

    Tyson makes the best videos on this channel. Clear and concise. And he doesn't make me feel as though I'm getting sold something for a change. Nicely done.

  • @paulevensen2322
    @paulevensen2322 Рік тому +4

    Great video Tyson! We're happy to provide our CitriSurf products and technical expertise to anyone who is interested in safe and environmentally friendly stainless steel passivation. -Your Friends at Stellar Solutions

  • @MurkinYuh
    @MurkinYuh Рік тому

    Love the videos that feature Tyson, he's the man! Always so clear and concise! Appreciate every video you guy release, there's always something I can apply how I do things in the shop.

  • @trevorgoforth8963
    @trevorgoforth8963 Рік тому +2

    It’s not even 8AM and I already something new today! Thanks Tyson, great video!

  • @davew4304
    @davew4304 Рік тому +9

    I don’t know why but I’m actually able to pay attention when Tyson and Barry makes a video

    • @barrysetzer
      @barrysetzer Рік тому

      I dont know why but whenever Dave W comments, I am actually able to read it 😂😂😂

  • @travisjarrett2355
    @travisjarrett2355 Рік тому +1

    Nice Tyson! Anything you can do to bring processes in house will save money and many times a headache. I can still smell that fire!

  • @ryanclarke2161
    @ryanclarke2161 Рік тому

    Great vid Tyson, you've got a lovely voice for this sort or work and a great pace and way of explaining things.

  • @AeroenginnerJosh
    @AeroenginnerJosh Рік тому +12

    A more simplified way of stating what passivation does, is the removal if the ferrous layer of material for the components surface. Often preformed on materials with a high chrome-nickle alloy, once the iron is removed the chrome and nickel is left exposed which has greater corrosion resistance. It is also important to note that for most large OEMs you will require outside accreditation from both the OEM and an external verifiers such as NADCAP.

  • @donniehinske
    @donniehinske Рік тому +2

    Good video dude! I never knew how this is done!! thats super cool to see

  • @paulkraus4799
    @paulkraus4799 Рік тому

    Always love your videos Tyson , and how you break it all down in simplicity

  • @12erplays39
    @12erplays39 Рік тому +1

    Thanks for the Video, I never worked with Stainless and also didn't know you had to do this after machining. Learnd something new today💪
    Barry awesome as allways

  • @jeremymatthies726
    @jeremymatthies726 Рік тому +1

    Hey Tyson, awesome job buddy on explaining this process. I had never heard of it being a thing for aerospace parts but makes sense. Its been a loooong time since I last did chemistry lol.

  • @FamTech.
    @FamTech. Рік тому +6

    Love your video's guys ceep on going!🎉😊

  • @Autonate_42
    @Autonate_42 Рік тому +2

    I love Barry in the background 😂

  • @dirtboy896
    @dirtboy896 Рік тому +3

    Always love to see a Tyson video. Man he has come a long way

  • @shortbus
    @shortbus Місяць тому

    What a great video sir! I'll be subscribing for sure!

  • @465maltbie
    @465maltbie Рік тому +9

    You dont talk about testing procedures to prove the passivation? If you do another video about the paperwork please include that also. Thanks for bringing this up. Charles

    • @danl.4743
      @danl.4743 Рік тому

      Did you read what it said on the document he showed? No need for verification.

    • @anthonyfrey9707
      @anthonyfrey9707 Рік тому +1

      ​@@danl.4743 Have you ever done work for the military. Just because a product states in their literature that it meets a particular standard does not mean that it's acceptable. In the standard, there is also a test requirement or multiple requirements that must be met in order to prove that the standard has been met. It is your job as the supplier to your customer to able to verify that the standard has been met.

  • @user-di6ve8ds8w
    @user-di6ve8ds8w Рік тому

    U give me new insight
    That makes my latheutube channel better than yesterday
    Thank you!

  • @danl.4743
    @danl.4743 Рік тому +1

    I don't know why but I laughed more than I was expected to, when you said "it has an x in the name". 🤣

  • @tech-utuber2219
    @tech-utuber2219 Рік тому +2

    Samwell Tarly performing passivation on Valyrian Steel.

  • @21mejia25
    @21mejia25 Рік тому

    Now I know what Passivation is! Thanks!

  • @vonpredator
    @vonpredator Рік тому +14

    For the rest of the world. 120F to 160F = 49C to 71C. 🤓

  • @AwestrikeFearofGods
    @AwestrikeFearofGods 9 місяців тому

    Nice demo. Do you water-rinse in between the cleaner and the acid? I didn't see that step.

  • @Imlibe1
    @Imlibe1 Рік тому +1

    Tyson u're the best!! 👍

  • @skjetnis
    @skjetnis Рік тому +3

    Man I love the huge ass lab coat

  • @Michael49637
    @Michael49637 Рік тому +2

    Tyson for president!

  • @willbe7442
    @willbe7442 Рік тому

    I love tysons videos.

  • @peterCheater
    @peterCheater Рік тому

    Did you ever get NADCAP for the outside processing you took in housw?

  • @NinjaPooop
    @NinjaPooop Рік тому

    Great video! Is heating the solution a requirement? Let’s say I don’t have a heater, could I just leave it overnight?

  • @RPrice_OG
    @RPrice_OG Рік тому +1

    Passivation isn't just for aerospace. If you are a home brewer or even a professional brewer then you may want to passivate all your pretty stainless stuff. I did this a couple years ago and it was extraordinarily hard to find someone to sell and ship the acid to me. I hope that this product will be available to hobbyists at some point.

  • @MattOGormanSmith
    @MattOGormanSmith Рік тому

    There are OTS kitchen devices with stainless tanks and redundant boil-dry protection. Maybe a rice cooker or a kettle would be a good size for you (not talking to the Titans here, unless they go to an industrial kitchen shop). Some of them will have suitable thermostats for that 120-160F range too.

  • @Berkana
    @Berkana 4 дні тому

    Would a sous vide machine work for that water heating step?

  • @clutchboi4038
    @clutchboi4038 Рік тому +3

    Thank you for this! I weld stainless steel pipes for water filtration systems and have been wanting to build my own passivation tank.
    But since you are going into stuff besides exclusively CNC machining, I was wondering if y'all have thought about doing plate bending with a cnc press brake? I just got one for my business and am still learning how to set it up.

  • @mlt3258
    @mlt3258 Рік тому +1

    Nice!

  • @mrbimsky
    @mrbimsky Рік тому

    Im not pro, but can i use baking powder + water for passivation?

  • @mjodr
    @mjodr Рік тому +1

    Even though citric acid seems safe because everyone loves to use cute photos of oranges and downplay it like "hey, what could go wrong?", concentrated "industrial grade" citric acid products like this and Citrol are SERIOUS stuff. They are one of the best solvents I could possibly find in weeks of research. They aren't exactly splash it around and get it in your eyes and mouth kind of stuff.

  • @darikmatters8866
    @darikmatters8866 Рік тому +1

    come on.. we want to see the Swiss machine turn out a shiny stainless passifier for the big baby in the lab coat.. Way to go Tyson, its been a while since I saw one of your videos..

  • @protector7886
    @protector7886 Місяць тому

    Does nitric acid work better to passivate stainless steel vs citric acid?

  • @VenturiLife
    @VenturiLife Рік тому

    That ending though.. haha

  • @Vankel83
    @Vankel83 Рік тому

    Did you dump the Citric Acid down the drain? Or di you put in a holding drum like bad coolant to be picked up and dispose of properly.

    • @danl.4743
      @danl.4743 Рік тому +4

      No. He added sugar to it and he keeps it in the fridge for hot days.

  • @myszkoscielna7522
    @myszkoscielna7522 Рік тому +1

    Great video, Tyson!

  • @runcycleskixc
    @runcycleskixc 2 місяці тому

    It would be nice to show what the passivation did to the steel part, apart from looking shiny. E.g. resistance to a salty solution overnight at high temps etc.

  • @jameslmorehead
    @jameslmorehead Рік тому

    How about passivization with phosphoric acid such as Ospho? I use Ospho all the time for any iron item that is bare iron.

    • @NoctisIgnem
      @NoctisIgnem Рік тому

      That only works for bare iron, stainless needs stronger acid

  • @dutchr4zor
    @dutchr4zor Рік тому

    Can you do a video on dimensionally stable anodising of aluminium?

  • @Azalea__Rose
    @Azalea__Rose Рік тому

    Does passivation alter the final dimension at all? like a coating might for example

  • @billmcleangunsmith
    @billmcleangunsmith Рік тому

    You were using 17-4, but does it also improve corrosion resistance on 300 series stainless?

    • @mjodr
      @mjodr Рік тому

      You can do this on lots of materials. I've actually done it on aluminum before using a slightly different process. I'm not doing aerospace certified stuff mind you.

    • @NoctisIgnem
      @NoctisIgnem Рік тому

      I do this professionally, we use nitric acid on stainless.

  • @eeeeweeezeee
    @eeeeweeezeee Рік тому

    Props to Tyson for not using the break room microwave for the science demonstration like I would have.

    • @barrysetzer
      @barrysetzer Рік тому +1

      Beahahaha that reminds me of one time we almost boiled a part in methylene chloride in a crock pot in our office (pre-Titans). And then i read the MSDS and realized we would all die lol

  • @klasjanzen1165
    @klasjanzen1165 Рік тому +1

    Waiting for the electro plating
    Since Barry did the anodizing, I was like: oh, I wish he did electro plating on carbon steel

    • @barrysetzer
      @barrysetzer Рік тому

      We are all over it Klas! Stay tuned

  • @kevinkc3onohelijeepworld953

    Any chance we are going to see a 10-20kw fiber laser metal cutting ?? 😊

  • @thelastgs-pian9965
    @thelastgs-pian9965 Місяць тому

    isnt stainless steel rust proof so why passivate , will this work on mild steel?

  • @hamzanawaz7945
    @hamzanawaz7945 Рік тому +1

  • @jenspetersen5865
    @jenspetersen5865 Рік тому +1

    Why not just use a Sous Vide stick for heating and you get circulation at the same time

  • @AlessioSangalli
    @AlessioSangalli Рік тому

    Hello, would this be useful after TIG welding?

    • @dragerx001
      @dragerx001 Рік тому

      tig welding put an oxide layer over welded joint and will cause it rust over time if not passivated.

    • @AlessioSangalli
      @AlessioSangalli Рік тому

      @@dragerx001 so it's a yes?

  • @africantwin173
    @africantwin173 5 місяців тому

    E330 for my beer Tanks.

  • @Yourmommaluvsme
    @Yourmommaluvsme Рік тому

    Yaassssss Tyson! Cherry Brahhhh, cuz

  • @KB-dd9xr
    @KB-dd9xr Рік тому

    Citric acid is used for skin peels so I would at LEAST wear gloves and rinse off well after this. Save your skin some surface burns!

  • @satchelsieniewicz5824
    @satchelsieniewicz5824 Рік тому

    its not a induction heater its a immersion heater. dont mean to be annoying all the best

  • @enjoyorgano
    @enjoyorgano Місяць тому

    Stainless steel is not resistant to acid. Why do we use acid to do passivation ? Do you need to wash is with a basic solution after the passivation ?

  • @raynerfpv2471
    @raynerfpv2471 Рік тому

    I would sign up for a class given by Professor Tyson 😂

  • @cdrom1070
    @cdrom1070 Рік тому

    lol be careful with those heaters. You know what they do, I had one that started bubbling because of corrosion. So what happens if they get a breach in the vessel, then you have water enter the inside, turn into steam, and cause a steam explosion. 1ml of water expands to like 4 liters of steam IIRC. I have seen pictures of aquariums that looked like they had a fire cracker inside of them. I suggest you use a hot plate and a glass non chinese lab beaker... any chemicals mildly corrosive are no bueno for that POS aquarium heater. Glass beakers are super nice so long you are gentle.

    • @cdrom1070
      @cdrom1070 Рік тому

      and I dunno if that is the same type of heater but you should be aware of the thermal mass of the heater. Basically its the same as a motor in a blower tube, if you turn it off abruptly and turn off airflow and measure the temp it will go up because there is latent heat inside of the thing that comes out, so normally stuff runs air for a while after it turns the motor off so it can cool down right. Those heaters will over-heat if you remove em from the bath abruptly and thermally stress them. The procedure is to turn it off and leave it in the bath for like a while. They suck.

    • @cdrom1070
      @cdrom1070 Рік тому

      you might think the 160 temp is low so there is no risk, but the watt density of the heater is heavy, meaning that the actual inside of the heater is pretty damn hot given the small surface area of the thing. I am telling you get a hot plate and beaker b4 that bull shit goes off on u

  • @SuperTommieNL
    @SuperTommieNL Рік тому

    A simple float switch with low water power cut off would have prevented the fire. 50 bucks or so

  • @jenspetersen5865
    @jenspetersen5865 Рік тому

    It is amazing to see Tyson's development from clearly having a lot of autistic traits, to really increase his social skills.
    Great example!

  • @timrussell1559
    @timrussell1559 Рік тому

    So, a person can have themselves a thriving and profitable business by soaking metal parts in warm orange juice? Sign me up!

  • @BigT89
    @BigT89 Рік тому

    NadCap accreditation

  • @yoyobah1862
    @yoyobah1862 Рік тому +2

    If you do this regularly it would be a good investment to buy a Sous Vide machine, they're not expensive.

  • @anwaryousaf4237
    @anwaryousaf4237 2 місяці тому

    Fire .... ha ha and you are telling workshop owners to do passivation by themselves.

  • @chauvinemmons
    @chauvinemmons Рік тому

    Thought you guys had a nasty experience doing plating and decided not to be doing that kind of thing anymore.

    • @TITANSofCNC
      @TITANSofCNC  Рік тому +1

      We talk about our mistakes in the video and how to prevent them