Annex Cube test after rail tramming

Поділитися
Вставка
  • Опубліковано 11 вер 2024
  • Getting closer...
    Tramming in the rails makes machine much more quiet and less vibration.
    Annex cube test for baseline.
    Seams are not right, non smooth surface/rough/jagged/out of place filament. Some corners not as crisp as I like. The issue I keep seeing is that when I increase PA, the seams get wider and more corner bulge. Less pa and the corners look much better, but lost the edge. Seems predictable.
    Overall it's a well crafted cube.
    Changing to a Capricorn bowden tube to see if a little tighter filament path will help. If this won't work(I have never used Capricorn in that location), I may put a sherpa extruder on and see if any change in performance.
    ABS, 265C, .015PA external/internal, .010PA everything else.