It is either T-initial or T-actual and not T-nominal in API 510.T-nominal is for API 570.Nice lecture!
For determining Corrosion rate, is it allowed to use nominal thickness as initial or previous thickness ?
initial but if no readings(CMLs) are taken it will have to be used as pervious also
Why do you emphasize indicating that there is no corrosion in the weld seam, if were corrosion in the weld seam do the equation of mínimum thickness required or the evaluation need to change?
Very Good knowledge
How to take allowable stress value (s).
It is provided to you in problem. However, that can be found on ASME II Part 4
How can I enroll in the API 570, 510
Thank you so much👍🏼👍🏼👍🏼
Nice
Thanks
It is either T-initial or T-actual and not T-nominal in API 510.T-nominal is for API 570.Nice lecture!
For determining Corrosion rate, is it allowed to use nominal thickness as initial or previous thickness ?
initial but if no readings(CMLs) are taken it will have to be used as pervious also
Why do you emphasize indicating that there is no corrosion in the weld seam, if were corrosion in the weld seam do the equation of mínimum thickness required or the evaluation need to change?
Very Good knowledge
How to take allowable stress value (s).
It is provided to you in problem. However, that can be found on ASME II Part 4