TIG Aluminum Setup and Settings

Поділитися
Вставка
  • Опубліковано 21 жов 2024
  • TIG Aluminum Setup and Settings is a video I made to answer the questions I keep getting. Hopefully this sheds some insight into getting your TIG dialed in!
    For Fabrication Inquiries, or for one on one Welding lessons email me at 5thstreetfab@gmail.com
    Check out my Patreon account at / 5thstreetfab
    Or visit my website at 5thstreetfab.comUse My coupon code to get 5% off of HTP Welders! (except Invertig 313) FIFTHST5%
    Here's my Affiliate link for the My HTP Invertig 400! The best TIG welder I've ever used!
    usaweld.com/co...
    My HTP Invertig 221! Best machine for the home hobbiest
    usaweld.com/co...
    usaweld.com/co...
    HTP Invertig 313!
    usaweld.com/co...
    MYe HTP Pro Pulse 220! Crazy pulsed MIG welder!
    usaweld.com/pr...
    here's my affiliate link for the welding coupons!
    weldmetalsonli...
    coupon code 5THSTREETFAB at checkout for 10% off. You can use this code for any order, not just a one time use!
    Here's a list of my Affiliate links! They don't cost you any extra but Amazon sends me a kick back of anyone that buys something through me. These are all tools that I personally use or have used and definitely suggest!
    HTP's Welders
    usaweld.com/?r...
    Evolution saw amzn.to/3fM5lYg
    Bandsaw amzn.to/39qeNQ0
    Optrel welding hood amzn.to/36iPYDx
    Speedglas Hood amzn.to/33uFrn4
    Jackson Fixed shade hood amzn.to/2HNGIxM
    123 blocks amzn.to/36kI7pc
    4" belt sander amzn.to/3mma5WZ
    Stripping wheel amzn.to/2KapN4x
    F Clamps! amzn.to/2JcdeKS
    40 Grit flap discs amzn.to/39teQKK
    Speed Square amzn.to/3lk7M5i
    Automatic center punch amzn.to/3o2YFIf
    My favorite Angle Grinder amzn.to/37flZMc
    Welding pliers amzn.to/2Jinpxn
    Bench Grinder amzn.to/3o7uShv

КОМЕНТАРІ • 209

  • @5thStreetFab
    @5thStreetFab  5 років тому +49

    Hey Guys Ive been getting a lot of questions about set up for aluminum so hopefully this helps!

    • @FrequencyOfThought
      @FrequencyOfThought 5 років тому

      Hey brother Im about to start a channel as well. Glad to see you starting out trying to help people.

    • @5thStreetFab
      @5thStreetFab  5 років тому +1

      @@FrequencyOfThought right on dude and thanks bud

    • @KillaCowboy
      @KillaCowboy 5 років тому

      What's your welding machine?

    • @scotchlobster6599
      @scotchlobster6599 5 років тому +1

      Thank you very much for these videos.

    • @soldieroftoughlove7635
      @soldieroftoughlove7635 10 місяців тому

      9:28 what needs to go up?

  • @Skeetmgeett
    @Skeetmgeett 5 років тому +26

    It's nice learning aluminum from someone who clearly knows AC. Good to see you back. I wish a certain company (cough HTP) would get you a fancy new tig welder for more aluminum videos, total no brainer htp.

    • @5thStreetFab
      @5thStreetFab  5 років тому +1

      Thanks dude! That would be awesome! Hopefully they see it our way!

  • @fredrico373
    @fredrico373 4 роки тому +2

    This is The Video off all UA-cam certified mechanical, thank you very much!! I've been trying to find this information for a long time.

  • @1navynasa2
    @1navynasa2 5 років тому +2

    Brother, thank you for this tutorial and explanation, what a difference!
    I'm welding aluminum for a long time and most of the time got good results, never thought about playing with the balance... good lesson :)
    Thank you!

  • @parikapustina1398
    @parikapustina1398 3 роки тому +1

    What did you change to get a better weld each time? You didn't describe

  • @LifeInHyrule
    @LifeInHyrule 3 роки тому +1

    Great video well done. Have you tried playing with gas flow settings as well? My experience has been upping the gas flow has a similar effect of increasing the cleaning percentage. Down side is more gas used, but the up side is the tungsten can maintain a sharper point keeping the arc more direct.

  • @bigj7807
    @bigj7807 4 роки тому +1

    Nice ! I have the same welder, good explanation of how frequency and balance actually affect the weld and what too look for when adjusting. Do you have a video on doing stainless ?

  • @taylorsmith9127
    @taylorsmith9127 Рік тому

    Pretty much on point man only tip I'd give is the crater cracks at the ends of ur weld slowly let off at then of a weld and swirl the torch that will get rid of those sometimes an extra dab is needed but those crater cracks are stress points

  • @FrustratedBaboon
    @FrustratedBaboon 2 роки тому

    Nice work 5th. I went away few years from welding but thinking to get back to it. I found a 25lbs aluminum CO2 tank and may cut it up into a go kart fuel tank for practice.

  • @JohnnyFaber
    @JohnnyFaber 5 років тому +1

    Thank you SO much for this video! The way you illustrate and explain things really really helped me get it! I was getting frustrated and after some of your vids I was stacking dimes!!!! So stoked about it! THANK YOU!!!!!

  • @elijahtaylor8351
    @elijahtaylor8351 5 років тому +2

    This video definitely helped me. I haven't welded aluminum with my everlast welder yet.

  • @senecalfab1487
    @senecalfab1487 5 років тому +1

    Awesome video explaining what I was seeing today my first time TIG welding and how to remedy it! Thank you!

    • @5thStreetFab
      @5thStreetFab  5 років тому +1

      That's awesome glad to hear it! Thanks for watching

  • @juanmangerita
    @juanmangerita 4 роки тому +1

    I have the same AHP welder and been having a hard time dialing it in... Do you use the torch that came with the welder??

  • @nicholaijerome7583
    @nicholaijerome7583 5 років тому +2

    Love the Lanthanated T! I don't weld much aluminum, but I have a project this week, thanks for the fresher!

  • @zeebee6702
    @zeebee6702 2 роки тому

    Very helpful video!!!
    Thanks for taking the time to explain some of your tips.
    I was struggling with some basics and you had some very good reminders.

  • @trailerpark187
    @trailerpark187 2 роки тому

    I always ran my balance on my syncowave at 10. But then I got a dynasty. Do you have a dynasty setting video? There's another guy on youtube but he charges a subscription fee to see his settings

  • @ion_canadianu
    @ion_canadianu 3 роки тому

    I have a lincoln 200 tig. It’s good for aluminium welding ?

  • @JP-yt3nk
    @JP-yt3nk 3 роки тому

    Fantastic tip on cleaning. Never thought of turning up the balance that high, was going by the cleaning zone around the bead and trying to keep that tight. That may be my issue, not just heat control.

    • @5thStreetFab
      @5thStreetFab  3 роки тому

      I had to turn it up so high because my machine was crapping out! Most machines would be fine around 65%-75%. After that you moght aant to try uping your gas flow!

  • @danssv8
    @danssv8 3 роки тому

    Thanks , so you using a pedal right??

  • @jrautofabwerksllc7556
    @jrautofabwerksllc7556 5 років тому +1

    I really appreciate the settings and tips and tricks for kids ❤️ help me weld aluminum

  • @Urchfab
    @Urchfab 5 років тому

    Good to see you back on the vids mate. great video as always.

    • @5thStreetFab
      @5thStreetFab  5 років тому

      Thanks Matt! I'm trying to find time!

  • @dreammakergarage1133
    @dreammakergarage1133 3 роки тому

    I learned so much from this video. Thank you so much for sharing.

  • @mattfuchs7626
    @mattfuchs7626 3 роки тому

    Great instructional video and process steps, very helpful!

  • @CarReporter12
    @CarReporter12 4 роки тому

    Hi.
    Great video.
    I am planning in buying a tig welding machine. My main use are building exhausts for my own cars so basically SS304/316 and titanium. But I might have to weld aluminum say for making brackets etc. but that will be very very rare, since I have shortlisted a AC/DC machine rated at 250amps. Will it be sufficient for alumium?

  • @kdk200
    @kdk200 4 роки тому

    How hot were you when doing the beads? If I did exact same thing it would be too hot to touch after 3 or 4 beads. I weld with 120amps. Is that too low and I'm slow?

  • @jonwatkins254
    @jonwatkins254 5 років тому

    Fabulous Video. Thank you for sharing the comprehensive and densely packed knowledge.

    • @5thStreetFab
      @5thStreetFab  5 років тому

      No problem bud! I really appreciate your comment.

  • @gaminacthemaniac6444
    @gaminacthemaniac6444 3 роки тому

    Would Thoriated tungstens work alright?

  • @thomasmonsenego-mo8140
    @thomasmonsenego-mo8140 4 роки тому

    What setup are you modifying during your different tries at more or less 10 minutes. The balance ?

  • @t54760
    @t54760 5 років тому +1

    I have that exact model AHP. Can you go into a little more detail on the problems you are having with it? I'm still relatively new to the aluminum side of welding and this is my first Tig machine. I guess what I'm trying to help determine is whether the issues are me or the machine. Another great video and Happy 2019 !

    • @5thStreetFab
      @5thStreetFab  5 років тому

      Ya im not sure exactly what's wrong. I think it has something to do with the alternating current being messed up almost like you need way more ac balance to correct it. But it makes it look like porosity is constantly burning out. The weld looks very grainy. And happy New year!

    • @t54760
      @t54760 5 років тому

      Initially, my aluminum welding was what I would have expected from a beginner and thought the learning process was going well. Then after a few months, I was welding some very thin wall aluminum square tubing and was having difficulty with arc starts. When I did get it going the arc would wander all over the place. This caused burn through. I Googled it and it turns out there is a set of points inside of our machines that wear and lose the proper gap with time. I followed the instructions, cleaned the points and reset the gap which was off quite a bit. This made it better but I still don't think I have the same performance as when I first got it. I would love to find a fix for this. The DC side still works great.

    • @5thStreetFab
      @5thStreetFab  5 років тому

      @@t54760 yep I did the same thing but still not as nice as I like!

  • @johnversluis3084
    @johnversluis3084 5 років тому +2

    Thank you !! so much this really helps setting up and a little more understanding how to setup AHP Happy New year !!

    • @5thStreetFab
      @5thStreetFab  5 років тому

      No problem bud and thanks for watching hopefully it'll help you out

  • @adamkwiatkowski4107
    @adamkwiatkowski4107 5 років тому +1

    I like blue tungsten.
    Do you have amazon link to tungsten ? Thx

  • @pitu66bat59
    @pitu66bat59 3 роки тому

    Legend in vídeo setting usage

  • @Brandon_Audi
    @Brandon_Audi 3 роки тому

    What series torch are you using in this video?

  • @farvatron
    @farvatron 5 років тому +1

    Thanks man this video is very helpful! I just bought my first welder, an ACDC TIG of course because why not!

    • @bigbothoee8617
      @bigbothoee8617 4 роки тому

      How you getting on with your welder ? Did you manage to setup ok ? I'm just waiting for my welder to turn up

    • @farvatron
      @farvatron 4 роки тому

      @@bigbothoee8617 it's easy as, you'll be fine just get some scrap and have a go :)

    • @bigbothoee8617
      @bigbothoee8617 4 роки тому +1

      @@farvatron swweeeeeet thanks

  • @theragingredneckhaulsoff6760
    @theragingredneckhaulsoff6760 3 роки тому

    Awesome video!

  • @danysperez-carrillo6630
    @danysperez-carrillo6630 3 роки тому

    Thanks for posting

  • @tommylud4324
    @tommylud4324 5 років тому +1

    What do you feel the balance would be if you cleaned with acetone and then a brush?

    • @5thStreetFab
      @5thStreetFab  5 років тому

      This AHP was on its last leg on my htp I'm around 75% dcen each machine is a little different that's why I like to do this test

  • @paulmattox
    @paulmattox 5 років тому

    Never really done aluminium. Would love to do more at work

  • @luisfernandotorres6980
    @luisfernandotorres6980 Рік тому

    Hi i take at picture of my tig and i like u teach ne how can setup for weld aluminum 1/8 sheet

  • @shaun2049
    @shaun2049 4 роки тому

    Thanks dude l find the settings harder than to weld just started welding ally’s hard

  • @weldnfab7136
    @weldnfab7136 4 роки тому

    How did you fit that cup on that torch ? Any adapter ?

  • @maxlindgren5986
    @maxlindgren5986 5 років тому +1

    Really nice video, i will go to my garage and try mixing with the settings and hopefully i will get much cleaner and better welds! :D
    This really helped me a lot!

  • @jordanhenningsen7938
    @jordanhenningsen7938 5 років тому

    Another great easy to follow video! Please keep them coming. I How do you cut your 2% lanthanated tungsten without cracking or splintering? I’m yet to find a easy quick way. I miss the quick snap of the thoriated tungsten.

    • @5thStreetFab
      @5thStreetFab  5 років тому

      I usually just hold it 45° at the edge of the belt sander until it cuts through most of the guys at work still snap the Tungsten but it splinters too much for me

    • @wonghunglo1
      @wonghunglo1 5 років тому +1

      i use small cutoff wheel on a dremel. snapping makes it splinter alot of times

    • @weldingjunkie
      @weldingjunkie 5 років тому

      Band Saw works great i use it on my swag table and cut them to any length,

  • @robertbasile4191
    @robertbasile4191 4 роки тому

    Hey, my machine (Hobart ez-tig 165) doesn't have frequency or balance adjustments. The cleaning line is basically right up against my bead. Having trouble making good beads. Any idea what I can do? (16 gauge aluminum)

  • @uniquemotivational1152
    @uniquemotivational1152 3 роки тому

    How much amps use for 1mm and 2 mm ss sheet

  • @octomulianto215
    @octomulianto215 2 роки тому

    How setting machine for thin aluminium, I have problem about it

  • @mytube3687
    @mytube3687 3 роки тому

    Is it possible to weld mild steel or stainless steel or Aluminium using Tig welding machine without gas?
    I mean is there special filling material which doesn’t need gas?(like MiG welder there’s gasless flux core wire you can use without gas for mild steel).

    • @Slouworker
      @Slouworker 2 роки тому

      No. Just stick weld it if you don't have gas.

  • @bigbothoee8617
    @bigbothoee8617 4 роки тому

    Perfect vid just what I wanted straight to point

  • @alec-s
    @alec-s 4 роки тому

    What changes very much between a pass and the other in those you made, is the sheet has heated up and you can get a faster and more precise fusion.... The real deal is the heat, sometime you should spend time in heating without sticking the rod in, just to increase the heat before you weld.
    For the heavier parts, ( 1,5 inches thick) sometime you need to fire preheat the part before start welding....

    • @5thStreetFab
      @5thStreetFab  4 роки тому +1

      I was showing the cleaning action nothing to do with the heat. I preheat most of my parts at work we weld anywhere from .063" to 2" thick. I only like preheat on parts 3/16" and over

  • @rtt931979
    @rtt931979 4 роки тому

    Hi! I have a Unimig 170A viper machine. My AC balànce adustment in the machine is only between 1-5 im confused and dont know what proper adjustment to select on it. By the way im just a beginner and im using Zirconated (white).

  • @whoisjohngalt11
    @whoisjohngalt11 4 роки тому

    I don't understand the point of balling the tip. Why not just round it off with the grinder instead of grinding to a point and then balling it off?
    By the way, I really appreciate that you did such a good job explaining the settings on this particular welder since I just picked one up. I'm going to run some beads with your settings tomorrow. I'm just getting started and I don't even know where to begin with settings.

    • @5thStreetFab
      @5thStreetFab  4 роки тому

      i like sharpening it first because its more consistent everytime. Thanks!

  • @boostedpower5417
    @boostedpower5417 3 роки тому

    Thanks dood I needed this!

  • @steveh9106
    @steveh9106 5 років тому

    Hi there, great video again for beginners, well explained and not to technical, with advice on Hardwear too, thanks for your time 😀

    • @5thStreetFab
      @5thStreetFab  5 років тому +1

      No problem bud and thanks for watching!

  • @turbotrana
    @turbotrana 5 років тому

    Good info there. How about setup for thick aluminium cast cylinder heads.I struggle on them (only played around on them) and have seen a pro do it easy. I need to play with a few settings.

    • @5thStreetFab
      @5thStreetFab  5 років тому +1

      All the thick castings I've done have been on a large transformer so I don't have any settings other than 60 Hz and a lot of cleaning. 4943 filler is awesome for it too

  • @FrequencyOfThought
    @FrequencyOfThought 5 років тому

    For the longest time I thought balling it was a bad thing and would regrind my tungsten but I found that the balling actually promotes the welding arc zone to be more predictable and the heat gets put into the material where you expect it versus a sharp tip that seems to pierce holes in the material. Hot and heavy versus controlled and medium pace. Considering aluminums melting point is lower than almost all other materials balling it makes good and complete sense.

    • @5thStreetFab
      @5thStreetFab  5 років тому

      Ya everyone has their own preferences. it's probably how you learn more than anything.

  • @PYWong-jq4pg
    @PYWong-jq4pg 5 років тому

    Awesome thanks! I always learn something useful on your channel. Gonna try those settings.

    • @5thStreetFab
      @5thStreetFab  5 років тому

      Thanks bud! I'm glad I can help. Good luck!

  • @johnmacmillan627
    @johnmacmillan627 3 роки тому

    Clearly shown. Thx

  • @davidcizek4024
    @davidcizek4024 5 років тому

    Hi Max …i Love your Videos i can learn alot of them …because i just started tig Welding and i Love it😀
    Most of all aluminum…keep up sharing your knowledge it is a BIG help for beginners like me👍
    Happy new year from Vienna Austria👍
    David

    • @5thStreetFab
      @5thStreetFab  5 років тому

      Thank you bud I appreciate it! I'll try to keep putting out videos! And happy New year to you too!

  • @markbroad119
    @markbroad119 5 років тому +1

    Nice, I've got that exact welder.
    Love that lil welder.

  • @oldscar6169
    @oldscar6169 4 роки тому +3

    AHP welder good instructional thank you

  • @mikerrr82
    @mikerrr82 5 років тому

    Hei. What tungsten for thin sheet alu and thick alu?

  • @cubegears
    @cubegears 3 роки тому

    what size torch is that? 17?

  • @tinybuilds2132
    @tinybuilds2132 7 місяців тому

    Hi
    What is the base metal that you are using

  • @andrewsigler2467
    @andrewsigler2467 5 років тому

    Ive always been told to use pure tungsten on aluminum. Is lanthenated better?

    • @5thStreetFab
      @5thStreetFab  5 років тому +1

      pure is what they used to run years ago on really old machines but now days there are way better choices like lanthanated

  • @v8consumption
    @v8consumption 5 років тому

    On my ahp I think the balance is backwards to most machines I generally keep it at 30% which gives less ball more sharp arc

    • @5thStreetFab
      @5thStreetFab  5 років тому

      Mines the same way but the AC was crapping out on me and I had to run super high balance to counteract it

  • @NSXTACY420
    @NSXTACY420 5 років тому

    What balance percentage did you end up on at that last nicest looking shiny bead? 40%?

    • @5thStreetFab
      @5thStreetFab  5 років тому +1

      It was actually something like 55% but I wouldn't trust it. This machine has been giving me big problems on AC

  • @chrisbec3313
    @chrisbec3313 4 роки тому

    Very informative! Thanks

  • @fastcash9799
    @fastcash9799 4 роки тому

    I have a Lincoln inverter machine do you still need to ball up the tunsten for aluminum?

    • @5thStreetFab
      @5thStreetFab  4 роки тому

      personal preference I usually put a small ball on my tungsten seems to help the cleaning action work better

  • @rattedbug5003
    @rattedbug5003 4 роки тому

    tHanks for the tips very helpful

  • @briansmedley9329
    @briansmedley9329 5 років тому

    What torch and hose is that? Can you link them please? I have the same ahp machine and looking for an upgrade over my stock torch. Any other upgrades you recommend to the machine?

    • @5thStreetFab
      @5thStreetFab  5 років тому

      its a ck superflex #9 from usaweld.com works great. any foot pedal like the ssc foot pedal especially is awesome

  • @DJCallitquits
    @DJCallitquits 5 років тому

    Learned a lot in this video!! Thanks!!

  • @hipairbrush1053
    @hipairbrush1053 2 роки тому

    great video

  • @HandWiredAmps
    @HandWiredAmps 5 років тому

    10:14 Vented back cap! I need one of those. 👍

  • @williamhayes136
    @williamhayes136 4 роки тому

    Sorry bro I'll keep my opinion to myself you do a good job

  • @ZILAwelds
    @ZILAwelds 5 років тому +1

    You need an htp 221 .... everything is “different” with a different machine .... the htp 221 LOVES 2% ceriated and has hard times arc starting with 2% lanthenated .... and the cleaning and penetration is “backwards” so 35% would be 65% ..... the inverter and the arc dynamic is so good that you easily weld at 70-75% on super clean material i even welded on 90%!
    And you have independent En+ and En- adjustments
    Water cooled guns will help you a lot with running high penetration numbers and high amperages on tungstens that “normally” would crack ....

    • @split150
      @split150 5 років тому +1

      I have a 221, and have noticed the same thing certain times when using Lanthanated tungsten. Always thought it was just me, or a bad ground or something. Never thought about it being the tungsten type. Thanks.

    • @5thStreetFab
      @5thStreetFab  5 років тому

      dude that sounds awesome! I know this machine is definitely on its way out as far as the ac balance is considered. thats crazy. Ive always wanted to mess with the independent en adjustments. Sounds so cool!

    • @ZILAwelds
      @ZILAwelds 5 років тому +1

      split150 on the 221 lanthenated is not a “good” choice. 2% lan has arc starting issues and 1.5% lan has a weird erosion pattern ....
      The funny thing is that in some European forum stel 221acdc customers ( which is effectively the identical machine ) have said that some equipment dealer or sales rep told them not to run lanthanated but encouraged them to run 2% ceriated and only if they cant get that run 2% thoriated ..... no lanthanated .... i found that pretty interesting ....
      And then if you put helium mixtures in the mix ..... arc starting suffers majorly in addition and arc stability suffers a little bit too.

    • @5thStreetFab
      @5thStreetFab  5 років тому

      @@ZILAwelds wierd I would figure tungstens would act similar from machine to machine. Very interesting

    • @ZILAwelds
      @ZILAwelds 5 років тому

      5th Street Fab all machines are a little bit different .... they all have their own idiosyncrasies ..... what works for one machine does not have to work for another machine ....

  • @jimmiemires2644
    @jimmiemires2644 4 роки тому

    What is "annoying" about a tight bead?

    • @5thStreetFab
      @5thStreetFab  4 роки тому

      I meant the noise of a high frequency around 200hz

  • @marcusmorgan1419
    @marcusmorgan1419 5 років тому

    Nice video, thanks for sharing with us newbs something useful.

  • @nameofdane
    @nameofdane 4 роки тому

    TONS of good tips! Thankyasir, gonna try and put some of these to use today.

  • @user9005
    @user9005 5 років тому +2

    I first thought zirconiated tungsten was the way to go but everyone is using lanthiated tungstens

  • @georgesmirnoff9751
    @georgesmirnoff9751 5 років тому

    Thanks brother! Man, I watch all the videos all the time but my welding still sucks, what should I do? ; )

  • @williamhayes136
    @williamhayes136 4 роки тому

    We all got our own opinion on this this smaller works for me and I would use pure Tung

  • @adamedgar5765
    @adamedgar5765 3 роки тому

    interesting comment about gas...other youtubers who are fabricators say that aluminium is not reactive to air environment. The gas is to protect the tungesten...not the aluminium.
    I innadvertantly ran out of gas the other day whilst TIG wedling some aluminium tubing and it didnt make any difference. The main way i knew it was out of gas was because of the sound difference but i kept on welding for quite a while to see what would happen...the weld was fine.

    • @5thStreetFab
      @5thStreetFab  3 роки тому

      Nope thats not correct. The gas does protect your tungsten but it also protects the molten aluminum. you dont need much coverage because as soon as the puddle solidifies the oxide layer that forms shields it from regular atmosphere. But until it solidifies you need argon coverage or you can get porosity and a dirty weld

    • @adamedgar5765
      @adamedgar5765 3 роки тому

      @@5thStreetFab i am wondering if you could do a video tig welding aluminium to show this with aluminium tubing and aluminium plate? I know with Mig welding i have never had any success without gas, i also thought TIG would be the same...so i was suprised to hear it can be done without.

  • @gyulakiss420
    @gyulakiss420 5 років тому

    Helo! The polariti change no change cables?

    • @RJB510
      @RJB510 5 років тому

      Leave cables as DCEN on Tig for alloy as well as most other tig welding types. Remember that alternating current effectively swaps your polarity anyway and the settings on your machine will most likely require your electrode to be connected to the machines negative terminal.
      You want to swap cables when using it as a straight dc stick welder.

  • @jakeowens1770
    @jakeowens1770 2 роки тому

    Looks good sounds like beginner

  • @WelcomeToTheMadness
    @WelcomeToTheMadness 5 років тому +1

    Learnt a little something...

  • @jamessonger3
    @jamessonger3 5 років тому

    What type of work do u do at ur job?

    • @5thStreetFab
      @5thStreetFab  5 років тому

      I do sub assembly for boats. A lot of fuel cells, crab pot davits, random boxes, hydraulic tanks basically anything that goes in or on a boat

  • @williamhayes136
    @williamhayes136 4 роки тому

    Switch to a smaller cup so you get a smaller heat line

  • @sgr5287
    @sgr5287 5 років тому

    Can I use this same settings using a HTP 221?

  • @starmanxv2331
    @starmanxv2331 5 років тому

    Well job . I have learn from you .💪

  • @ayazkhan-bm5uh
    @ayazkhan-bm5uh 5 років тому

    Nice video and information. Thank you
    one more information.
    Welding definition.

  • @chadandrews98
    @chadandrews98 5 років тому

    Thanks for good information

  • @reddyreddy2618
    @reddyreddy2618 Рік тому

    0:05 if the belt had grabbed a hold of that tungsten you could be in for an injury, don't angle in to the direction of a sanding belt people

  • @tysonhimself
    @tysonhimself 5 років тому

    Good tips thanks

  • @johnmacmillan627
    @johnmacmillan627 3 роки тому

    Thx

  • @pararescue88
    @pararescue88 5 років тому

    Perfect video

  • @geraldturkeyhunter
    @geraldturkeyhunter 5 років тому +1

    Pre heat your metal you kept welding on same piece over over til you hit the sweet spot pre heat it do same thing once

  • @davidswanson4437
    @davidswanson4437 4 роки тому +1

    Do the Ball, Be the Ball, but one doesn't need to. Cleanliness is next of godliness. A clean aluminum has a thin layer of aluminum oxide that needs to be removed with the positive side of the AC cycle, thus saving the tip. For the most part, even with 1" thick aluminum on a Miller Aerowave (350 amps, Tri-Mix 1/8" electrode, some balling, but not complete ball). Think about it. The positive side of the AC cycle removes the aluminum oxide instead of melting it (3,762°F melting temp). The electrode negative cycle melts the aluminum at 1,220°F. Helium gas ($$) and high amps are used on pure DCEN for aluminum when the cleaning ("cathodic etching") can not be tolerated. Remember Heliarc? If a sharp tip punches holes, turn down the amps - practice welding aluminum soda cans together (remember most machines HF start is with higher amps).
    ntrs.nasa.gov/archive/nasa/casi.ntrs.nasa.gov/20040139717.pdf
    "Because the electrons extract heat from the cathode {work piece} and deliver heat to the anode {electrode}, the welding process is considered to be more efficient when operated in “straight polarity,” when the torch electrode is negative, the workpiece positive, and electrons flow to the workpiece. Unless there’s a reason not to, welding torches are operated in the straight polarity mode. But there is a reason to weld in “reverse polarity,” where the electrons flow away from the workpiece: the cathodic cleaning effect. A high speed movie of the vicinity of a GTA weld pool in the reverse polarity mode will reveal a display of sparkling points of light, miniature explosions continually occurring all over the surface. This is thought to be caused by electrostatic breakdown of a thin surface oxide layer. The positive ions in the arc accumulate on the surface of the oxide layer and induce a balancing negative charge. If the oxide layer is thin, it doesn’t take a lot of charge to produce an electric field (volts per distance) big enough to cause the oxide layer to break down in a mini-explosion. Cleaned surface is distinct and visible around the crown of a weld made in reverse polarity. But to get the cleaning necessary to weld aluminum alloys one takes a hit in power available for welding, and the effective capability of the machine is reduced."
    Hope this helps,
    David

  • @williamhayes136
    @williamhayes136 4 роки тому

    Bro you ever want to hire someone let me know

  • @jcjimenez5327
    @jcjimenez5327 4 роки тому

    This is a great 👌👌👌

  • @traininggrounds9450
    @traininggrounds9450 5 років тому

    Just accept it with AC, it's balled up or it ain't welding. E3 and other harder tungstens don't ball up consistently to be good production rods for AC. Blue is better than purple and pink is better than blue when it comes to arc stability but I believe white to be the best tungsten for AC every time. Just get E3 for DCEN only and white for AC only and you'll make the best welds in both worlds.