    Please remember that this is an oversimplified version of what could be a much more complex formulation depending on the specific requirements, environmental regulations, and manufacturing processes involved.
    Ingredients:
    Liquid Rubber Base (e.g. Liquid Styrene-Butadiene Rubber (SBR)): 70kg
    Solvent (e.g. Toluene or another appropriate solvent): 25kg
    Fillers (e.g., Carbon Black): 1.5kg
    Plasticizers (e.g. Dibutyl phthalate): 1kg
    Curing Agents/Vulcanizing Agents (e.g., Sulphur): 1kg
    Accelerators (e.g., Tetramethylthiuram Disulfide (TMTD)): 0.5kg
    Antioxidants (e.g., N-(1,3-dimethylbutyl)-N'-phenyl-p-phenylenediamine): 0.5kg
    Stabilizers (if required)
    Colorants (if required)
    Please note that this is just a basic formulation and can be highly variable depending on the specific product specifications, the environment in which it is being used, local regulations, and the precise type of rubber. Also, the proportion of each ingredient might change to optimize the product for specific applications.
    In a real-world setting, the development of a commercial liquid rubber product would involve extensive research, testing, and compliance with industry safety and quality standards.
    Also, I should mention that the solvent and some other components in this theoretical formulation could be hazardous, both from a health and safety perspective and in terms of environmental impact. Therefore, always handle these materials with care, in a professional setting, with appropriate personal protective equipment, and in accordance with local laws and regulations.
    Disclaimer: This hypothetical formulation is for illustrative purposes only. Actual manufacturing should be performed by professionals following industry safety and quality standards, in compliance with all relevant laws and regulations, and after performing the necessary testing to ensure the product meets all required specifications.

КОМЕНТАРІ • 27

  • @abdullahaliabbasi
    @abdullahaliabbasi Рік тому +2

    I was watching for the formula, but overall video is also good...

  • @MuhammadKhan-nj8qq
    @MuhammadKhan-nj8qq Рік тому +1

    Wah kia baat hay, super.

  • @syedamjadalikazmi2796
    @syedamjadalikazmi2796 Рік тому +2

    ❤اسلام وعلیکم جواد صاحب سلامت رہیں.
    انڈین چینلز پر اس طرح کی پراڈکٹ دیکھی تھی اور اسکی ضرورت اپنے ملک میں بہت ھے اب آپنے اپنے چینل کی وساطت سے اسکو عام کردیا اسکے لیے بہت شکریہ. اباد رہیں.

  • @mufpower
    @mufpower Рік тому

    Very nice

  • @shahkhan8997
    @shahkhan8997 Рік тому

    You are an Angel

  • @muhammadnoor7854
    @muhammadnoor7854 Рік тому +1

    MashaAllah very good👍🤲🤲

    • @zageerajpoot648
      @zageerajpoot648 3 місяці тому

      Assalam-o-Alaikum
      Bhai video banayin Ac fan ko dc mein kaisay convert karin kam budget mein. Ap videos aysi banatay hain issi liay ap se request hai.

  • @khalidaziz9850
    @khalidaziz9850 Рік тому +1

    In video formula mentioned Rubber SBR. not P/ URETHANE.

  • @ptilongmarch8044
    @ptilongmarch8044 Рік тому +1

    میں آپ کی ہر ویڈیو دیکھتا ھوں

  • @amjad268
    @amjad268 Рік тому +1

  • @uzairghani5797
    @uzairghani5797 Рік тому +1

    Jawad Bhai yeah kitna Effective ha means Kitne degrees tak effect karay GA?

  • @khalidaziz9850
    @khalidaziz9850 Рік тому +1

    PU water base hy ya solvent base.

  • @kashifmehboob3748
    @kashifmehboob3748 Рік тому

    Wait, Wait, Wait.... If we put it's layer inside the tubeless tyre, and to apply further save a little solution in a tube (cosmetic cream tube etc) to make the punctures done effectively. Will it work??? As claimed alongation is 600X, provide strong bounding, long lasting, made of poly-urithene mean composition is also suitable for rubber. 🤔 🤓

    • @JawadFarooq
      @JawadFarooq  Рік тому +1

      No it will not work

    • @khalidaziz9850
      @khalidaziz9850 Рік тому

      water base PU doesnt work and solvent base PU will damage tube rubber.

  • @AbidKhan-ee8tf
    @AbidKhan-ee8tf Рік тому

    Assalam o Alakum jawad bhai aap achi or informative video banate hain
    Is company ke office ka number mil sakta hai shukria

  • @zaheerbandey7726
    @zaheerbandey7726 Рік тому +1

    Lahore mey is product k dealer ka address or number kya hey

    • @JawadFarooq
      @JawadFarooq  Рік тому

      Bahi video dobara dekhain, start main hi dia hua hai

  • @rashidahmad3287
    @rashidahmad3287 Рік тому

    اس کا فارمولا تو آپ نے بتایا ہی نہیں ۔

    • @JawadFarooq
      @JawadFarooq  Рік тому

      Video pori dekhain darmain main hi hai

    • @MuhammadDanish0
      @MuhammadDanish0 8 місяців тому

      Jawad bhai ye sab aik Sath dal k mixture ko kitne tk chalain

  • @adnanabbasi1630
    @adnanabbasi1630 Рік тому +1

    PU چائنہ ytong

  • @adnanabbasi1630
    @adnanabbasi1630 Рік тому

    اگر PU ہےتو Sandwich Panel بھی بناتے ہیں؟؟؟

    • @JawadFarooq
      @JawadFarooq  Рік тому

      kuch samjh nahi aa rahi app ki

    • @adnanabbasi1630
      @adnanabbasi1630 Рік тому

      @@JawadFarooq سر جواد، اصل میں PU POLYURETHANE ہی کی کمبینیشن سے SANDWICH PANEL کولڈ اسٹوریج کے کئے بنائے جاتے ہیں۔ اور یہ PU ہی خام مال ہوتا ہے۔ اور چائنہ سے آتے ہیں۔ پاکستان میں کوئی نہیں بناتا۔ یہی pu کو ریفریجرنٹ گیس کے ساتھ ریئکٹ کروا کر اعلی کوالٹی کے فوم (بیڈ فوم) بنائے جاتے ہیں۔ غالبا ytong کمپنی کا نام ہے۔