You still alive? No new post scare me. Also, adding heat to AP can send some of your gold into solution. So your AP/ Dillute Nitric mix could easily cause gold loss on heat. I would test that solution with stannous when you finish. If any golds in solution, SMB should drop it like normal. 🤔
Nonsense? The gold is still worth the same. Its not like you make more money because of using Nitric actually the opposite hecause most people over pay for nitric. When using AP uou can cut the time down to 3 days by using heat plus a pump to agitate the solution. Each process has its purpose and depending on the refiner one process may work better than another for someone. Never think something is nonsense because recovering the gold is the main purpose
Do the math, hes adding 68% nitric acid to however much water is in the beaker minus a little for the mass of the fingers, simple math gives you the answer from there
It varies. Do you have all older fingers like ISA or other similar ones basically early 90s and older, AGP and PCI will yield the least amount, late 90s newer. Than you have memory fingers, these can vary because the vast amount of knock off brands. This can all vary with how close you cut the fingers leaving little to no each green board behind means more fingers in one pound and the older something is most likely will have thicker plating and doing individual types like I stated will give you yield data if you want to buy on ebay
Nice job bro, glad to see you stil making a videos ;)
Is there a part two ?
You still alive? No new post scare me. Also, adding heat to AP can send some of your gold into solution. So your AP/ Dillute Nitric mix could easily cause gold loss on heat. I would test that solution with stannous when you finish. If any golds in solution, SMB should drop it like normal. 🤔
So much more efficient than that sit it in AP for a week or more nonsense. Good job.
Nonsense? The gold is still worth the same. Its not like you make more money because of using Nitric actually the opposite hecause most people over pay for nitric. When using AP uou can cut the time down to 3 days by using heat plus a pump to agitate the solution. Each process has its purpose and depending on the refiner one process may work better than another for someone. Never think something is nonsense because recovering the gold is the main purpose
AP on heat can send gold into solution. I imagine you can precipitate it from the AP solution normally with smb though 🤔
What percent is your dilute nitric acid?
Do the math, hes adding 68% nitric acid to however much water is in the beaker minus a little for the mass of the fingers, simple math gives you the answer from there
How may grams pure gold?
Jane Peacock 1-3 grams per pound of clean fingers ...
It varies. Do you have all older fingers like ISA or other similar ones basically early 90s and older, AGP and PCI will yield the least amount, late 90s newer. Than you have memory fingers, these can vary because the vast amount of knock off brands. This can all vary with how close you cut the fingers leaving little to no each green board behind means more fingers in one pound and the older something is most likely will have thicker plating and doing individual types like I stated will give you yield data if you want to buy on ebay
Uh...
Your not breathing the fumes are you🧟♂️
Fuck dude wear gloves for god's sakes... Nitric will fuck your day up FAST, especially out in the woods 🤨