Thank you so much Prof Dr Nishna Pradeep for such an elaborate explanation of the process. now I am able to link the whole process and understand. The pictures of all the key steps & videos made the whOle process so much easier to comprehend. I am very geatful. God bless you for your kind effort. Many thanks
THANK YOU MAAM FOR SHARING THIS WITH US , FOR THAKING THE BURDEN TO MAKE SUCH VIDEO , ITS BEAUTIFULLY EXPLAINED AND NOW THE THEORY IS PIECE OF CAKE ITS REALLY HELPFUL AND NOW ITS EASY TO UNDERSTAND SUCH AN IMPORTANT TOPIC . THANK YOU MAAM
Thanks for such an elaborate explanation of the process. Picture of each step and a short video clip of the process all were very helpful in understanding the process
Very interesting video,,but my question is when i melt nickel chrome there is always a white membrane covering the molten metal.whrn i released the spring it splash in different direction and the metal frame makes some pores and fissures. So my question is what is that white layer covering the molten alloy and how can i remove it???
hi..you let the invested wax pattern to cool off after the burn out furnace ...and then you put it in the casting machine? cos i see you take it with your hand ..meaning that its cool..nothing happens?? no contraction? or problems? cos the metal goes in hot..and the invested is cool..thanks for the help
layering of ceramic over the metal coping is done step by step .It involves condensing and firing opaque porcelain, dentin and enamel porcelain.The appropriate shades of these powders are selected and used during ceramming to obtain the final shade and translucency .Moreover characterisation and stains can be incorporated before the final glazing to mimic natural tooth as close as possible.
Hello..I have important question...& I hope u answer me....if I have 5 bonding artificial teeth... Can I add a new artificial tooth to be bond with them? Or it's impossible?
i'm a dental tech/ ceramist in IL. She has the basics but her procedures are not good at all. OMG never get a crown done by her, sorry but I see this case failing
Thanks alot... Now only iam able to picturise what i read in theory..
Thank you so much Prof Dr Nishna Pradeep for such an elaborate explanation of the process. now I am able to link the whole process and understand. The pictures of all the key steps & videos made the whOle process so much easier to comprehend. I am very geatful. God bless you for your kind effort. Many thanks
thank you😊
@@prosthodonticsmadeeasy سلام
Thank you so much mam, I swear tomorrow I have my uni exam and I never ever in life understood this until I saw this video today 🙏🏻
Thank you so much mam..live demo is more superior than ppt and theories..hats off mam
Glad to hear that
Wow...finally understood the procedure..
More than amazing❤
THANK YOU MAAM FOR SHARING THIS WITH US , FOR THAKING THE BURDEN TO MAKE SUCH VIDEO , ITS BEAUTIFULLY EXPLAINED AND NOW THE THEORY IS PIECE OF CAKE
ITS REALLY HELPFUL AND NOW ITS EASY TO UNDERSTAND SUCH AN IMPORTANT TOPIC . THANK YOU MAAM
Thanku so much mam,for such deep view of casting 🙏🙏🙏
Thanks for such an elaborate explanation of the process. Picture of each step and a short video clip of the process all were very helpful in understanding the process
thank you🥰
Thanks a lot madam. Was having a very difficult time understanding casting procedure, this video came as a savior.
thank you😊
Thank you for your efforts..it helped alot
Thankuu so much ma'am 😇😇your videos are very helpful for us
❤❤
Thank you mam..u explained really well
Really useful for me thank u maam ❤❤❤
thanks for this amazing video prof !!
Good teaching
Best! Thank you ma'am
Great video thank you 👍❤
Very interesting video,,but my question is when i melt nickel chrome there is always a white membrane covering the molten metal.whrn i released the spring it splash in different direction and the metal frame makes some pores and fissures.
So my question is what is that white layer covering the molten alloy and how can i remove it???
Thank you very much for the informative video
Can we do porcelain coping on white metal (which is only for metal crown)??
This is interesting. Thank you very much!!!! But my question is should we polish the metal frame after oxidation treatment in the furnace????
so useful videos for freshers like me. ma'am what was that liquid mixed into investment plaster?
Please mam do make video on impression materials❤
Thank u so much for this video also❤
Thank you so much mam for this video.
hi..you let the invested wax pattern to cool off after the burn out furnace ...and then you put it in the casting machine? cos i see you take it with your hand ..meaning that its cool..nothing happens?? no contraction? or problems? cos the metal goes in hot..and the invested is cool..thanks for the help
yea that's what i was wondering
Mam can use plaster of Paris for ring making silver
too weak and when you burnout the wax, pop gonna show alot of cracks . better buy investment plaster
@@rushabhsoni407 yes I can try it's
@@rushabhsoni407 bahot weak rahata hai ye investment powder hi sahi hai par pata nahi kaha milta hai
👌👌great video
Great
Wow great work dr .but your lab
ha ha i know..we have a lot of limitations here..shall try to upload a perfect sequence of casting procedure soon..thank you for the feedback😊
@@prosthodonticsmadeeasy oh
Very informative Class mam
thank you😊
thank you so much Dr ... Good explanation
Most welcome!
thank you so much 😍😍😍
I know that Ring quenched in water is not good for good metal fitting.
Great !! Dr
thank you😊
Direct water chance bridge work rocking seating issues
Hello, thank you so much! Could you tell me where did you study to become tooth mechanic? I would like to start learning this profession in India. :)
Thank you maam for this video... But I have a doubt... How does the chosen color of the crown will make?
layering of ceramic over the metal coping is done step by step .It involves condensing and firing opaque porcelain, dentin and enamel porcelain.The appropriate shades of these powders are selected and used during ceramming to obtain the final shade and translucency .Moreover characterisation and stains can be incorporated before the final glazing to mimic natural tooth as close as possible.
Thankuhh mam .. do more video mam plz💝
thank you dear🥰really hoping to cover as many topics as possible for budding dental students.
Mam can investment Powder and plaster of Paris deference
Yes
Hello..I have important question...& I hope u answer me....if I have 5 bonding artificial teeth... Can I add a new artificial tooth to be bond with them? Or it's impossible?
It is possible but it take but it not viable alternative
Very informative. Can you please tell Which textbook do you recommend to learn the theory of this process?
Super
Thanks
Kerala ?
How to connect with you mam???
After casting direct water no problem
Thank u mam
Pl wait after casting precool time 30 minutes
WOW
Laksiridental lab dummaladeniya west Wennappuwa
Good morning mam
Ok
👍
i'm a dental tech/ ceramist in IL. She has the basics but her procedures are not good at all. OMG never get a crown done by her, sorry but I see this case failing
Hello mam can i get ur number ..? I want to learn lab procedures.
Thank you so much mam ❤