I've tried Cam auto Pro, Anson, Wurth, Dent fix and Collision Glue Systems. Nothing holds better or releases cleaner than CGS solar blitz. Give them a try you won't regret it.
I got mine off the Snap-on truck. Anyone who sells frame rack equipment should be able to get them. Looks like you can order them through their web site too. www.moclamp.com/TacPull.html
Really nice technique with the plate pull, too bad you had to add filler. I believe every body shop needs a PDR guy on call to get that panel level so filler, sanding and painting would not be required.
Yeah but thats how you kill body man making money along with the painter. With how insurance companies are going they are screwing us every chance they get. There is no money in big tow in wrecks anymore unless you're doing high end cars at a show with clean rooms and proper equipment
Great job brother what temperature did you heat the quarter before you put clam hand temperature did you have to leave it before you star pulling thank you great tips 👍🏽
Quality work! Awesome job!!
Thanks for the support!
Awesome ideas. Thanks
What were you pulling with - other end with the chain?
Quality repair! Did you sand the tab at all or just leave the original finish on it?
The tab was prepped by grinding it with 80 grit and cleaning it with isopropyl.
💪💪💪💪
Nice, I’m shopping around for some glues to try at my work, have you tried any other brands?
I've tried Cam auto Pro, Anson, Wurth, Dent fix and Collision Glue Systems. Nothing holds better or releases cleaner than CGS solar blitz. Give them a try you won't regret it.
Great stuff! Can we purchase these plates at a bodyshop supply possibly?
I got mine off the Snap-on truck. Anyone who sells frame rack equipment should be able to get them. Looks like you can order them through their web site too.
www.moclamp.com/TacPull.html
Amazon has them
Perfect job. Respect to you)
Thank you very much!
Nice repair
Thanks buddy!
Really nice technique with the plate pull, too bad you had to add filler. I believe every body shop needs a PDR guy on call to get that panel level so filler, sanding and painting would not be required.
I agree! In the future I feel that its going to be common.
Yeah but thats how you kill body man making money along with the painter. With how insurance companies are going they are screwing us every chance they get. There is no money in big tow in wrecks anymore unless you're doing high end cars at a show with clean rooms and proper equipment
@@mattsvoboda2639 there is still plenty of work for the body man.
Solar Blitz glue ? Pretty good stuff. Nice pulling job.
Thank you we appreciate your comment
What is the name of the glue ? Can we buy it at Amazon ?
It is solar blitz and you can get it at collisiongluesystems.com thanks for your comments
Great job brother what temperature did you heat the quarter before you put clam hand temperature did you have to leave it before you star pulling thank you great tips 👍🏽
I heat the panel up to 200°f then wait until the glue has cured to a uniform temperature.