SPONGE IRON MAKING TECHNOLOGY RELATED QUESTIONS

Поділитися
Вставка
  • Опубліковано 16 січ 2025

КОМЕНТАРІ • 22

  • @sudiptakundu877
    @sudiptakundu877 2 роки тому

    Sir please make more videos ..your are best 🥰🥰❤️❤️

  • @rajeshpatel9701
    @rajeshpatel9701 2 роки тому

    Thanks you sir .

  • @mtsidhuu9672
    @mtsidhuu9672 11 місяців тому

    Sir Magnatite ko kaha use karta he

  • @rupeshsripati
    @rupeshsripati 4 місяці тому +1

    if Fe(t) is 63.35 then Oxygen will be 63.35 x 0.429=27.177, but in your calculation oxygen is 22.55 ,,,,,please clarify it.

    • @trueindian4887
      @trueindian4887 Місяць тому

      You are right …. It’s a simple calculation…48/111.7=0.4297

  • @shayankumar2752
    @shayankumar2752 2 роки тому +1

    Sir lobe ka airvolume kaise calculate karenge?

    • @rk.information5172
      @rk.information5172  2 роки тому

      Lob ka succation area nikalkar velocity se multiplay karne se air volume nikalta he

  • @subhamsoni7124
    @subhamsoni7124 2 роки тому

    Sir boice acic ka test kaise karte ha jo raming mass me used karte hai i please explain

  • @dhananjaykiran7679
    @dhananjaykiran7679 2 роки тому

    Sir lobe ka air volume kaise calculate karenge

  • @सत्यऔरविजय
    @सत्यऔरविजय 2 роки тому +1

    Plz sir ho ske to white board ka use kijiye usme jada achha samjh aur dikhega bhi
    And video ko view bhi jada milega

    • @rk.information5172
      @rk.information5172  2 роки тому

      i am not any professional video maker its just information for how want to learned about dri making information and grow and clear doughts.

  • @Jaga-s9d
    @Jaga-s9d Рік тому

    Wustite means kya he sir

  • @dhananjaykiran7679
    @dhananjaykiran7679 2 роки тому

    Sir ye coal ash composition kya hai

  • @aslamafzal2448
    @aslamafzal2448 2 роки тому

    Sir ji information is good but camera posing is not proper we cannot see the calculation correctly

  • @bhagawatkaushik6038
    @bhagawatkaushik6038 Рік тому

    Different fe(m) and MZ

  • @kiranrayaprolu424
    @kiranrayaprolu424 Місяць тому

    You are confusing all fe t is a chemical compostion moisture and blue hematite is a physical analysis how can you mix all

  • @bimalmandi9720
    @bimalmandi9720 2 роки тому

    Kiln inside mein kyu ring ho jata hai,
    Kiln inside mein ring na ho iskeliye kya karna parega

    • @rk.information5172
      @rk.information5172  2 роки тому

      Air,qrt and coal through profile ko perfect karna pade and low ash coal use karna padega, or yadi High ash coal he to acceration formation to hoga but slow hoga yadi aap coal and temp profile ko proper set karte he and use according iron feed ko