Base, hiranik adjustment, edge narrowing after hardening. I do it on a belt sander. Blade aso 0.3mm. The final sharpening and geometry is on the arato stone. Another polishing of some stones. It's here on video somewhere. If the customer wishes, everything can be done manually. Just the file before hardening and the stones after hardening. However, it is necessary to pay something extra for such work. It is expensive. because it takes a lot of time. .
excelent work, all explained in detail, LIKE !
For me to afford genuine polishing stones is out of the question. So its very nice to see how to do it with commonly available materials.
the nugui you used worked very well. that tanto is nice!
Thank you. Blade to nice. as co-Bizen. I buy nugui from Namikawa heibei. Commonly available, a mix of different types. .
Great work , do you buy the Nugui in powder form also I see there is black red and green , do I need them all
sangat bagus karya seni ini
Thank You
very interesting
so if you finished the polishing the blade wil be sharp, too? or is there an other sharpening process?
Base, hiranik adjustment, edge narrowing after hardening. I do it on a belt sander. Blade aso 0.3mm. The final sharpening and geometry is on the arato stone. Another polishing of some stones. It's here on video somewhere. If the customer wishes, everything can be done manually. Just the file before hardening and the stones after hardening. However, it is necessary to pay something extra for such work. It is expensive. because it takes a lot of time. .
刃ズや、地ズやの裏張りに、ガアデ又は水ペイパーを貼ると滑り止めになります、一度試して下さい、日本より、頑張って下さい
Do you use hot vinegar?
no, chlorid ferum , hot water, jitekko
there are english subtitles
What kind of sandpaper do you use?
Przecież to oczywiste. Papier wodny dobrej klasy np. do lakieru samochodowego.
Smirdex, in woter (red)