12 micron polyester is always equal to 19 micron ld . so to calculate the consumption of ld simply 50 ÷ 19= 2.63 so 1 kg polyester film ke saath 2.63 kg ld lagega
Sir 2 ply job 12/12/40 6 col job Solvent less lam After printing minimum kitna weight gain ana chahiye. Aur sir final weight hamesha input se kam ho raha hai.
Phone I use for shooting :
amzn.to/2THgLpx
Tripod I use for shooting :
amzn.to/3j1gKFx
Thanks for watching
Ink costing ke bare mein batayi
which are low cost synthetic rubber adhesives in the market?
Sir how to calculate cost of adhesive used in poly with aacuracy
Very nice video sir
Dear sir
Good evening
Sir Printing ke bare me bhi khuch bata dijiye kaise colour ka combination hota h.
Hi sir
Helpful knowledge
how to do costing of self adhesive tapes
Sir pp flim ki dincity kiya hoti hai or jese 240,gaj hai to kiya hogi
Or parar ka gsm 50 hai to dincity kiya hogi
Please bataye
Density fix hoti h sbhi polyester ki aapko kiska pta Krna h
Superb video sir next video kab aata sir
Very good sir.
Sar lamination mein ispekling kiske Karan aata hai please sir comment
Sir is there is any software for per costing and post costing
Sir how to calculate ratio percentage by valume
Nomosker sir
thanks a lot
very very important issue.
sir please solvent less gsm how caculate comes auto gsm on screen.why? please sir advice
helpful
how to do costing of self adhesive tapes please explain
Sir
Please use Mike. Thank you for the knowledge.❤️
Very nice vedio . Thank you for making vedio
Sir namskar ,mujhe 100kg pet me,50macon ki poli तो kitni lgegi, nechurl ,saej 655 srl sbdo me batae adsiv kitna lgega
12 micron polyester is always equal to 19 micron ld . so to calculate the consumption of ld simply 50 ÷ 19= 2.63 so 1 kg polyester film ke saath 2.63 kg ld lagega
46÷16.8×100=273.80kg ld lagegi
9kg adisive
@@arpitsaxena4245solventless main tention kaise deta hai please bataye bhai
CAC 1511A hardner me 50% solid content hota hai plzzz reply 🤔
Yes, haa hota hai.
Please vai aap ka number dijiye
Sir, what is 59 value of name ??
Sir jee ek bar ink costing ka video daliye na
Sir 1.5 gsm h to total solvent kitna kg ho share video
Tq sir
Sir ecl k bare me btaye
Sir lamination troubshooting par video banae
Thanks sir
Sir machine par gsm kaire Seth kare
Solvent less adhesive formula .By volumes and metering calculation
How to calculate adhesive gsm from printed laminate
Thanks you sir
Sirji muji lamination adhesive and stickers adhesive ka formaltion bathoge plz
👌👌👌👌👌👌👌
Dear sir, lamination Machine taper tension technical definition bataiye
Sir Poly film dart calculate farmula please share video
Good afternoon sir
please put video 2 ply raw material cost video
Sir aapse contact kese hoga pls btaye..
Contact me on 8401670508
Natural rubber adhesive manufacturing process
Sir 2 ply job
12/12/40
6 col job
Solvent less lam
After printing minimum kitna weight gain ana chahiye.
Aur sir final weight hamesha input se kam ho raha hai.
CALCULATION WRONG....! 5900*2.5/14.75 = 1000 KGS COMING SIR. BUT, U HAVE MENTIONED 100KGS *59 =5900 PET. PLS CORRECT ME IF I AM WRONG
51500 meter h 2.8 gsm
English translation please 😢
Wrong hai sir, aur aasan tharike സെ simple method me calculate kar saktha hai
Very wrong information
Solid % as well as calculation
Kisi ko pata hai vinyl base inks me kitna solid content hota hai
Please refer every ink manufacturer TDS so you can understand.
Adhesive ka viscosity Kitna rakhna chahiye plzz explain
@@shivammishra2391 its deepened upon solid contents of adhesive please refer TDS.
Aapka naya Vedio kab aane wala hai
Wrong
Sir ji aap ka WhatsApp no my help mi
Thanks sir
Thanks sir