  • @kensendelofski3761
    @kensendelofski3761 4 роки тому +1

    Thanks for the video enjoyed it, i used to do body work in the 70s. At that time lead was 9 cents a pound. That's just scrap lead. Any why thanks again

  • @SQ_og
    @SQ_og 12 років тому +1

    Great work but what is that tinning and tell us about the cloth.

  • @lyellblogg2130
    @lyellblogg2130 2 роки тому

    I’ve seen OS videos on “lead loading” (USA and UK) and they have used a tinning compound that is painted on and then heated, is that another item that is not available in Aus?

  • @snakeoil24
    @snakeoil24 11 років тому +1

    What kind of tourch head is that?

  • @rayarsenault1618
    @rayarsenault1618 8 років тому

    of course being in Australia you might hear about it in 50 years!

  • @rayarsenault1618
    @rayarsenault1618 8 років тому

    You thats outlawed?